Diesel engine gear failure

The failed diesel engine was installed on the fishing boat, with the power of 198 kW and the working speed of 750 rpm. After 700 hours of operation, the gear of the rudder gear broke and the diesel engine was damaged. The gear material is 45 steel, and the...