The gear material of the edw-300-l drum shearer is 17crnim06e steel. The heat treatment process is quenching and tempering, and it breaks during operation. The macro fracture morphology of gear teeth is shown in Figure 17, with the macro characteristics of fatigue fracture, and the electron micrograph is shown...