Witness-Based Simulation of Drive Pinion Gear Machining

I investigated the machining process of drive pinion gears used in coal shearers because these components are among the most critical wearing parts in the equipment. The reliability and timely supply of pinion gears directly affect the continuous operation of high-yield and high-efficiency coal mines. In recent years, the demand for coal energy has continued to grow, and many mines have increased their annual output from about five million tons to approximately ten million tons. This increase has imposed higher requirements on the reliability, maintainability, and delivery punctuality of shearer parts. Among these parts, pinion gears are especially important because they transmit large torque and traction forces, engage with the scraper conveyor pin rack, and withstand substantial cutting reaction forces. As a result, pinion gears are prone to failure, difficult to replace underground, and often supplied as part of a drive assembly. The manufacturing cycle of pinion gears is long, and delays in their supply can cause production stoppages and significant economic losses. Therefore, I focused on the machining process of pinion gears and used Witness, a discrete-event simulation platform, to model, analyze, and optimize the production process.

My research began with a field investigation of the actual machining system. I found that the production of pinion gears is a typical discrete-event dynamic system. The system consists of multiple machine groups, buffers, labor resources, and part flows. The processing routes are fixed, but the system contains random factors such as processing time variations, machine failures, setup adjustments, and labor availability. Traditional empirical analysis and simple calculations can identify obvious capacity shortages, but they cannot easily capture the interactions among machines, buffers, and part flows. Therefore, I adopted system simulation as the main methodology. I built a Witness model of the pinion gear machining process, validated it against observed data, and then used the model to evaluate alternative improvement scenarios.

System simulation foundations. System simulation is a method that uses models to imitate the behavior of real-world systems. It is especially useful when analytical solutions are difficult or impossible to obtain. A discrete-event system is one in which the state variables change only at discrete points in time when events occur. In the pinion gear machining system, events include the arrival of a part, the start of machining, the end of machining, the movement of a part into a buffer, and the completion of a batch. The simulation clock advances from one event to the next, and the system state is updated accordingly. The main elements of a discrete-event simulation include entities, attributes, activities, and events. In my model, the entities are the pinion gears in various stages of production. The attributes include processing time, priority, and routing. The activities include machining, heat treatment, and inspection. The events include part arrival, machine loading, machine unloading, and part transfer.

The utilization of a machine group is a key performance measure. I calculated it as follows:

$$
U_m = \frac{T_{busy,m}}{T_{total}} \times 100\%
$$

where \(U_m\) is the utilization of machine group \(m\), \(T_{busy,m}\) is the total busy time of machine group \(m\), and \(T_{total}\) is the total simulation time. The throughput of the system is another important measure. For a machine group with \(N_m\) identical machines, the theoretical maximum throughput can be estimated as:

$$
Q_{max} = \frac{N_m T_{total}}{T_{cycle}}
$$

where \(T_{cycle}\) is the cycle time per part. However, because of blocking, starving, failures, and setup times, the actual throughput is usually lower. I also used the average work-in-process (WIP) and the average time in system to evaluate the performance of the pinion gear production line. These measures are defined as:

$$
\bar{W} = \frac{1}{T_{total}} \int_0^{T_{total}} W(t) dt
$$

$$
\bar{T} = \frac{1}{N} \sum_{i=1}^{N} T_i
$$

where \(\bar{W}\) is the average WIP, \(W(t)\) is the number of parts in the system at time \(t\), \(\bar{T}\) is the average time in system, \(N\) is the number of completed parts, and \(T_i\) is the time in system for part \(i\). When I ran multiple independent replications, I also computed the sample standard deviation:

$$
S = \sqrt{\frac{1}{N-1} \sum_{j=1}^{N} (X_j – \bar{X})^2}
$$

where \(X_j\) is the performance measure from replication \(j\), and \(\bar{X}\) is the sample mean. These formulas helped me quantify the variability in the simulation output and make reliable comparisons among alternative configurations.

Witness software and modeling elements. Witness is a simulation environment designed for discrete-event systems. It provides a set of graphical elements that can be combined to represent a manufacturing system. The main element types I used include machines, buffers, labor, and parts. A machine element represents a processing resource. It can be a single machine, a batch machine, an assembly machine, or a production machine. A buffer element represents a storage area for parts. A labor element represents a human resource or a shared resource that performs operations. A part element represents the entities that flow through the system. Witness also provides rules and functions that define how parts are pulled, pushed, and processed. The software supports animation, reporting, and experimentation, which makes it suitable for modeling pinion gears and other complex manufactured components.

I modeled the pinion gear machining system with the following element types:

Element name Type Quantity Description
Duanjian Part 1 Raw material for pinion gears
rechuli Machine 1 Heat treatment group
chechuangzu Machine 4 Lathe group
xianqiege Machine 4 Wire-cut group
gunchizu Machine 2 Hobbing group
mochuangzu Machine 3 Grinding group
mochizu Machine 2 Gear grinding group
qiangognzu Machine 1 Fitter group
b1 Buffer 1 Input buffer for lathe group
b2 Buffer 1 Input buffer for wire-cut group
b3 Buffer 1 Input buffer for hobbing group
b4 Buffer 1 Input buffer for grinding group
b5 Buffer 1 Input buffer for fitter group

The model also included a variable element to record the number of completed pinion gears and a time-series element to monitor the system state. The layout of the simulation model followed the actual process route. I defined the part arrival as passive, meaning that raw pinion gears enter the system when they are pulled by the first machine group. The routing of each pinion gear followed the sequence: heat treatment, lathe group, wire-cut group, hobbing group, grinding group, gear grinding group, and fitter group. After the fitter group, the completed pinion gears left the system.

Machining process of pinion gears. The pinion gears used in coal shearers are typically classified into cycloidal-tooth pinion gears and involute-tooth pinion gears. Because involute pinion gears are more widely used and because their production suffers from more bottlenecks, I selected an involute pinion gear as the object of study. The typical machining route for an involute pinion gear is: forging, normalizing and high-temperature tempering, rough turning, aging, semi-finish turning, wire-cut rough tooth profile, hobbing semi-finish tooth profile, fitting, carburizing, semi-finish turning, hardening, finish turning, grinding, wire-cut internal spline, gear grinding, and fitting. The process involves multiple heat treatments and cross-workshop transfers. The detailed operations and machine times are shown in the following table.

Operation Content Machine Time (min) Number of machines
05 Turning: rough turning surface CW6180 11 h 20
10 Heat treatment: aging and stress relief Box furnace 12 h 9
15 Turning: semi-finish turning surface CY-K6180 5 h 30 min 20
20 Wire-cut: rough cutting involute tooth profile CTWQ800Z 75 h 25 min 14
25 Hobbing: semi-finish tooth profile YA31200K 31 h 2
30 Fitting: tooth profile chamfering Fitter 1 h 2
35 Heat treatment: carburizing Pit furnace 110 h 5
40 Turning: semi-finish turning outer surface CY-K6180 4 h 30 min 20
45 Heat treatment: hardening Multi-purpose furnace 16 h 2
50 Turning: finish turning with grinding allowance CY-K6180 2 h 20
55 Grinding: finish machining outer surface MKW28125 5 h 3
60 Turning: finish turning inner surface CY-KX6180 2 h 20
65 Wire-cut: internal spline CTWQ800Z 27 h 30 min 14
70 Grinding: finish grinding tooth profile P1200G 9 h 15 min 2
75 Fitting: deburring Fitter 1 h 2

After grouping the operations by machine type, the total processing time for one pinion gear can be summarized as follows.

Process group Lathe group (20) Wire-cut group (14) Hobbing group (2) Grinding group (3) Gear grinding group (2) Fitter group (2) Heat treatment group
Time (min) 1500 6175 1860 270 555 120 8280

The total processing time per pinion gear is the sum of these values. I used these data as the basis for the simulation model. The pinion gears move through seven main machine groups: lathe group, wire-cut group, hobbing group, grinding group, gear grinding group, fitter group, and heat treatment group. Each pinion gear must complete all seven stages in a fixed sequence. The processing times used in the model are shown in the following table.

Operation Lathe group Wire-cut group Hobbing group Grinding group Gear grinding group Fitter group Heat treatment group Total
Time (min) 1500 6175 1860 270 555 120 720 11200

These values represent the nominal processing times. In reality, there are setup times, adjustment times, breakdowns, and operator availability constraints. I incorporated these factors into the Witness model through machine attributes, labor rules, and breakdown distributions.

Modeling objectives and detailed design. The main objective of my simulation study was to evaluate the current production capacity of the pinion gear machining line, identify bottlenecks, and propose improvement measures. I set the simulation time to one month, assuming 30 working days and 8 working hours per day. Therefore, the total simulation time was \(30 \times 8 \times 60 = 14400\) minutes. I used a warm-up period to reduce the effect of initial conditions. For each scenario, I performed multiple independent replications with different random number streams. The performance measures included throughput, machine utilization, average WIP, and average time in system. I also monitored buffer contents and labor utilization.

The detailed design of each machine group followed the actual routing and processing rules. For example, the lathe group was modeled as four single machines with a cycle time of 12 hours. The input rule was based on buffer content:

$$
\text{Input: if } NPARTS(b2) \ge 4 \text{ then pull from } b1 \text{ else wait}
$$

$$
\text{Output: push to } b2
$$

The wire-cut group was modeled as four single machines with a cycle time of 25 hours. Its input rule was:

$$
\text{Input: if } NPARTS(b3) \le 2 \text{ then pull from } b2 \text{ else wait}
$$

$$
\text{Output: push to } b3
$$

Similar rules were applied to the other machine groups. The hobbing group had two machines, the grinding group had three machines, the gear grinding group had two machines, the fitter group had one machine, and the heat treatment group had one batch machine. The heat treatment group was modeled as a batch processor because multiple pinion gears can be treated simultaneously in the furnace. The buffers were modeled as first-in-first-out queues. The labor element was assigned to operations that require manual adjustment, such as fitting and inspection.

Model verification and validation. I verified the model by checking the logical structure, the input-output rules, and the animation. I also validated the model by comparing the simulation results with observed data from the actual production line. For example, I calculated that the lathe group should complete its first pinion gear at approximately 37 hours. I set the simulation clock to 37 hours and ran the model. The animation showed that the first pinion gear had just been pushed into the wire-cut buffer. The variable that counted completed pinion gears changed to 1. The report statistics confirmed that the lathe group had completed one operation and that the wire-cut buffer contained one part. The relevant statistics are shown in the following tables.

Buffer name Total in Total out Now in Max
b2 2 1 1 0
b3 3 0 0 0
Machine group % Idle % Busy No. of operations
rechuli 4.98 95.02 15
chechuangzu(1) 50.25 49.75 4
chechuangzu(2) 51.24 48.76 3
chechuangzu(3) 57.21 42.79 3
chechuangzu(4) 62.69 37.31 3
xianqiege(1) 23.38 76.62 1
xianqiege(2) 29.35 70.65 1
xianqiege(3) 35.32 64.68 1
xianqiege(4) 41.29 58.71 1
gunchizu(1) 74.13 25.87 1
gunchizu(2) 80.10 19.90 1
mochuangzu(1) 95.52 4.48 2
mochuangzu(2) 100.00 0.00 0
mochuangzu(3) 100.00 0.00 0
mochizu(1) 95.40 4.60 1
mochizu(2) 97.76 2.24 0
qiangognzu 99.00 1.00 1

The validation results showed that the model was able to reproduce the actual behavior of the pinion gear machining system. The random variations in processing times were consistent with the observed data. After confirming the model, I proceeded to run the simulation for the full 14400-minute period.

Output analysis of the original model. I ran the original model three times with the same random number stream and a simulation time of 1440 minutes to observe the short-term behavior. The statistics for the raw pinion gear parts are shown in the following table.

Name No. entered No. shipped No. rejected W.I.P. Avg W.I.P. Avg time Sigma rating
Duanjian1 31 0 210 31 20.35 157.58 0.00
Duanjian2 31 0 210 31 20.30 157.45 0.00
Duanjian3 31 0 210 31 20.33 157.52 0.00

I then computed the sample mean, standard deviation, and variance of the key performance measures over three independent replications. The results are shown below.

Name No. entered No. shipped W.I.P. Avg W.I.P. Avg time
Mean 31 210 31 20.33 157.52
Standard deviation 0 0 0 0.046 0.179
Variance 0 0 0 0.002 0.032

The average WIP was 20.33 pinion gears, and the average time in system was 157.52 minutes. The average time in system accounted for about 37% of the total simulation time. The highest machine utilization was the hobbing group, reaching 71.26%, while the lowest was the heat treatment equipment, at only 0.88%. The grinding group and the hobbing group had very low utilization, below 10%. Among the machine groups, only the lathe group had a non-zero blocking rate, and it was very high, around 86.3%. This was mainly due to the passive part entry mode, the large number of lathe machines, the short processing time, and the low failure rate. Both the animation and the statistical analysis showed that buffers b2 and b3 contained many pinion gears. Buffer b2 held 18 pinion gears at the moment of observation, with an average of 12. The average dwell time of pinion gears in b2 was 102 hours. This indicates that most of the waiting time occurred in b2. The wire-cut group had a setup time that accounted for 20.77% of its cycle, and the waiting time for workers to perform setup accounted for 24.84%. From the perspective of idle rates, the wire-cut group and the hobbing group were the main bottlenecks. The system operated under a general load, and the simulation output was 43 pinion gears per month.

Optimization by changing quantity factors. Based on the original model results, I identified that the wire-cut group and the hobbing group were the main capacity constraints. I first tested an optimization scenario in which I increased the number of machines in the bottleneck groups while keeping the processing times unchanged. In optimization scenario one, I increased the number of lathe machines to 2 and the number of wire-cut machines to 6. I ran the model seven times independently for 14400 minutes. The simulation interface changed accordingly, and the utilization results are shown in the following table.

Name 1 2 3 4 5 6 7 Average
Lathe group 66.21 66.09 66.22 66.14 66.13 66.18 66.14 66.16
Wire-cut group 66.35 66.26 66.43 66.29 66.32 66.40 66.23 66.33
Hobbing group 96.88 96.81 96.94 96.83 96.85 96.90 96.79 96.86
Grinding group 76.71 76.71 76.74 76.75 76.70 76.65 76.76 76.72
Gear grinding group 9.85 9.85 9.84 9.87 9.85 9.86 9.85 9.86

The results showed that the utilization rates were 66.16%, 66.33%, 96.86%, 76.72%, and 9.86% for the lathe, wire-cut, hobbing, grinding, and gear grinding groups, respectively. The hobbing group was still above 90%, indicating a high load. The output increased to 51 pinion gears per month.

In optimization scenario two, I further increased the number of hobbing machines to 3. I kept the other parameters the same and ran the model seven times. The utilization results are shown in the following table.

Name 1 2 3 4 5 6 7 Average
Lathe group 74.61 74.65 74.62 74.69 74.66 74.68 74.59 74.64
Wire-cut group 75.76 75.72 75.77 75.74 75.78 75.77 75.69 75.75
Hobbing group 55.08 54.98 55.02 54.98 55.03 55.09 54.92 55.01
Grinding group 55.37 55.38 55.46 55.38 55.35 55.42 55.34 55.39
Gear grinding group 84.72 84.68 84.70 84.72 84.76 84.72 84.58 84.70

The utilization rates were 74.64%, 75.75%, 55.01%, 55.39%, and 84.70% for the lathe, wire-cut, hobbing, grinding, and gear grinding groups, respectively. The output increased to 58 pinion gears per month. This showed that increasing the number of bottleneck machines can significantly improve throughput, but it also requires additional investment.

Optimization by changing time factors. I also investigated whether reducing processing times through advanced equipment and improved methods could alleviate the bottlenecks. I first reduced the processing times of the lathe group, wire-cut group, hobbing group, grinding group, and heat treatment group while keeping the number of machines unchanged. The revised processing times are shown in the following table.

Operation Lathe group Wire-cut group Hobbing group Grinding group Gear grinding group Fitter group Heat treatment group Total
Time (min) 1200 5600 1660 270 555 120 680 10085

In optimization scenario one for time factors, I changed the processing times of the main machine groups and kept the number of machines the same. I ran the model seven times for 14400 minutes. The utilization results are shown below.

Name 1 2 3 4 5 6 7 Average
Lathe group 98.28 98.24 98.31 98.25 98.27 98.29 98.32 98.28
Wire-cut group 80.14 80.54 80.54 79.98 80.00 80.27 80.67 80.31
Hobbing group 63.66 64.40 64.00 64.01 63.57 63.83 64.07 63.93
Grinding group 8.18 8.21 8.19 8.21 8.23 8.19 8.20 8.20
Gear grinding group 98.28 98.24 98.31 98.25 98.27 98.29 98.32 98.28

The utilization rates were 98.28%, 80.31%, 63.93%, 8.20%, and 98.28% for the lathe, wire-cut, hobbing, grinding, and gear grinding groups, respectively. The lathe group and the gear grinding group were still at high load. The output did not improve significantly.

In optimization scenario two for time factors, I further reduced the processing times of all machine groups except the heat treatment group. The utilization results are shown in the following table.

Name 1 2 3 4 5 6 7 Average
Lathe group 98.50 98.47 98.53 98.48 98.56 98.61 98.59 98.53
Wire-cut group 57.82 56.93 57.18 57.23 57.90 57.51 57.20 57.40
Hobbing group 64.57 64.18 63.90 64.07 64.62 64.70 64.24 64.33
Grinding group 8.17 8.22 8.14 8.16 8.18 8.16 8.13 8.17
Gear grinding group 98.50 98.47 98.53 98.48 98.56 98.61 98.59 98.53

The utilization rates were 98.53%, 57.40%, 64.33%, 8.17%, and 98.53% for the lathe, wire-cut, hobbing, grinding, and gear grinding groups, respectively. The lathe group and the gear grinding group remained at high load. Although the output increased slightly, the bottleneck problem was not fully resolved. The high cost of advanced equipment also made this option less attractive.

Combined optimization of quantity and time factors. Based on the previous results, I concluded that changing quantity factors alone or changing time factors alone could not fully solve the bottleneck problem. Therefore, I tested a combined optimization scenario. I used the improved processing times and increased the number of machines in the bottleneck groups. Specifically, I increased the number of lathe machines to 2, wire-cut machines to 6, hobbing machines to 3, and kept the other machine groups unchanged. I ran the model seven times for 14400 minutes. The utilization results are shown in the following table.

Name 1 2 3 4 5 6 7 Average
Lathe group 67.57 67.61 67.46 67.53 67.54 67.50 67.58 67.54
Wire-cut group 66.48 66.54 66.44 66.41 66.52 66.43 66.47 66.47
Hobbing group 39.39 39.43 39.36 39.34 39.37 39.35 39.33 39.37
Grinding group 39.35 39.33 39.35 39.37 39.31 39.34 39.38 39.35
Gear grinding group 84.71 84.76 84.71 84.69 84.67 84.65 84.72 84.70

The utilization rates were 67.54%, 66.47%, 39.37%, 39.35%, and 84.70% for the lathe, wire-cut, hobbing, grinding, and gear grinding groups, respectively. The output increased to 62 pinion gears per month. This combined approach balanced the system load and improved the throughput significantly.

Comparison of simulation results. I compared the original model and the optimized scenarios. The following table summarizes the key performance measures.

Scenario Lathe utilization (%) Wire-cut utilization (%) Hobbing utilization (%) Grinding utilization (%) Gear grinding utilization (%) Monthly output (pinion gears)
Original High High High Low Low 43
Quantity scenario 1 66.16 66.33 96.86 76.72 9.86 51
Quantity scenario 2 74.64 75.75 55.01 55.39 84.70 58
Time scenario 1 98.28 80.31 63.93 8.20 98.28 —
Time scenario 2 98.53 57.40 64.33 8.17 98.53 —
Combined 67.54 66.47 39.37 39.35 84.70 62

The comparison shows that increasing the number of machines in the bottleneck groups improved the output, but it also created new bottlenecks. Reducing processing times alone did not resolve the bottleneck because the lathe group and the gear grinding group became highly loaded. The combined optimization achieved a more balanced utilization and the highest output. The monthly processing capacity increased from 43 pinion gears to 55–60 pinion gears, an improvement of approximately 35%. The average WIP and average time in system were also reduced, indicating smoother material flow.

Implications for pinion gear production. The simulation results provide several important insights for the production of pinion gears. First, the wire-cut group and the hobbing group are the primary bottlenecks in the original system. Increasing their capacity can quickly improve throughput. Second, the heat treatment group has a high utilization in some scenarios, and its batch nature can cause long waiting times. Scheduling heat treatment operations carefully is important. Third, the layout and transfer times between workshops affect the overall performance. Reducing cross-workshop transfers and improving the layout can shorten the average time in system. Fourth, the use of advanced gear grinding machines can reduce processing times and improve precision, but the investment cost must be justified by the increase in throughput and quality. Fifth, the simulation model can be used as a decision support tool for capacity planning, scheduling, and process improvement.

Conclusions. I built a Witness-based discrete-event simulation model for the machining process of drive pinion gears. The model includes machine groups, buffers, labor resources, and part flows. I validated the model against actual production data and used it to analyze the performance of the current system. The original system produced approximately 43 pinion gears per month, with the wire-cut group and the hobbing group acting as bottlenecks. I tested several optimization scenarios involving changes in machine quantity, processing time, and a combination of both. The combined optimization achieved a monthly output of 55–60 pinion gears and improved the overall utilization balance. The simulation results showed that the model can accurately reflect the actual production process and can provide effective decision support for production management, process optimization, and system analysis. The use of Witness for modeling pinion gears and other complex components can help manufacturing enterprises reduce costs, shorten delivery times, and improve competitiveness. In future work, I plan to incorporate more detailed data on machine failures, operator schedules, and quality inspection, and to extend the model to include the entire supply chain of pinion gears.

Scroll to Top