I designed and analyzed a high-power, small-transmission-ratio spur face gear pair under severe space constraints. The central problem I addressed was not only to make a face gear pair fit inside a limited annulus but also to prevent the face gear from suffering edge contact, tooth-tip stress concentration, and eccentric load when the transmission ratio is small. In a conventional face gear drive, the contact path usually lies near the inner radius and pitch region; for a small-ratio face gear pair, the radial distance between the pitch circle and the mid-face-width can be large, so the load naturally migrates toward one side. I therefore treated the face gear pair design as a coupled geometry, modification, and installation-error problem. I used tooth contact analysis (TCA) and loaded tooth contact analysis (LTCA) to quantify transmission error, contact path, contact stress, root bending stress, and tolerance sensitivity. The final face gear pair achieved a contact area of about 86.5% of the working flank, a contact ratio of about 1.83, and acceptable stresses under the specified torque.

Space constraints and first layout decisions. I began with the available envelope. The face gear had to be placed between a minimum inner diameter of 187 mm and a maximum outer diameter of 250 mm, so the allowed face width was at most 31 mm. The mating cylindrical pinion could not exceed an outer diameter of 167 mm. These limits are severe for a face gear because a face gear usually needs enough radial room to avoid undercut near the inner radius and tooth pointing near the outer radius. I therefore expressed the basic face gear ratio as
$$i=\frac{\omega_2}{\omega_1}=\frac{z_2}{z_1}$$
where \(z_1\) is the number of face gear teeth and \(z_2\) is the number of pinion teeth. For the required small-ratio range, I considered \(i=0.695\) to \(0.927\). The transmitted torque at the pinion was \(T_1=1030.57\ \mathrm{N\cdot m}\). I applied an application factor \(K_A=1.1\) and a dynamic factor \(K_v=1.1\), so the torque used in the finite element and LTCA models was
$$T=K_A K_v T_1=1.1\times1.1\times1030.57=1246.0\ \mathrm{N\cdot m}$$
Because the pinion space was tight, I set its tip diameter equal to the largest permitted value for a candidate module and tooth number. With addendum coefficient \(h_a^*=1\) and clearance coefficient \(c^*=0.25\), the pinion tip diameter is
$$d_{a2}=m\left(z_2+2h_a^*\right)=m\left(z_2+2\right)$$
I used the condition \(d_{a2}\le167\ \mathrm{mm}\) to screen module and tooth-number combinations. In parallel, I estimated the face gear pressure angle at an arbitrary diameter \(d\) from the approximate relation
$$\cos\alpha(d)=\frac{m_n z_n\cos\alpha_n}{d}$$
where \(m_n\) is the normal module, \(z_n\) is the virtual tooth number, and \(\alpha_n\) is the nominal pressure angle. The inner and outer limits of the face gear were controlled by undercut and pointing conditions:
$$R_{\min}\ge R_{\mathrm{undercut}},\qquad R_{\max}\le R_{\mathrm{pointed}}$$
For a small-ratio face gear pair, the pitch radius of the face gear is close to the inner boundary, so the useful contact region tends to move inward. This is the main reason that a small-ratio face gear pair is prone to eccentric load. I selected a preliminary module of \(m=3.9\ \mathrm{mm}\), a pinion tooth number \(z_2=40\), and a face gear tooth number \(z_1=51\), giving a nominal ratio
$$i=\frac{40}{51}=0.7843$$
This ratio lies inside the required range and also satisfies the space constraints. I also evaluated several alternative modules. The tooth-number windows that I found are summarized in Table 1.
Table 1. Module and tooth-number screening for the small-ratio face gear pair.
| Module \(m\) (mm) | Pinion teeth \(z_2\) | Face gear teeth \(z_1\) range |
|---|---|---|
| 3.0 | 53 | 58 to 76 |
| 3.5 | 45 | 49 to 64 |
| 3.9 | 40 | 44 to 57 |
| 4.2 | 37 | 40 to 53 |
| 4.5 | 35 | 38 to 50 |
After screening, I selected the \(m=3.9\ \mathrm{mm}\) case because it offered a good balance between face width, bending strength, and the available pinion envelope. The preliminary face gear parameters are listed in Table 2. These values are not yet the final modified design; they are the geometric starting point that I used to expose the contact-path and eccentric-load problems.
Table 2. Preliminary small-ratio spur face gear pair parameters.
| Parameter | Value |
|---|---|
| Module \(m\) | 3.9 mm |
| Pinion teeth \(z_2\) | 40 |
| Face gear teeth \(z_1\) | 51 |
| Minimum inner radius from undercut \(R_{\min}\) | 95.34 mm |
| Maximum outer radius from pointing \(R_{\max}\) | 110.28 mm |
| Mid-face-width radius | 110.17 mm |
| Face gear pitch radius | 99.45 mm |
| Initial face width | 29.66 mm |
| Pressure angle range on face gear | 19.02° to 43.86° |
I also performed an initial calculation with a shaper cutter that had one more tooth than the pinion. That is a common way to introduce a tooth-number-difference modification into a face gear. The initial example is given in Table 3. The first TCA run showed that the contact points clustered near the inner radius of the face gear, close to the pitch circle. The outer part of the face gear tooth was barely loaded, and the tooth tip was at risk of edge contact. The stress field confirmed a strong eccentric load toward the inner side. This behavior is unacceptable for a high-power face gear pair because it reduces the effective contact area and raises local contact stress.
Table 3. Initial trial parameters for the face gear pair.
| Parameter | Value |
|---|---|
| Module | 3.9 mm |
| Pinion teeth \(z_2\) | 39 |
| Shaper cutter teeth \(z_s\) | 40 |
| Face gear teeth \(z_1\) | 51 |
| Pressure angle | 25° |
| Inner radius | 97 mm |
| Outer radius | 125 mm |
I then examined a tooth-number-difference modification with a one-tooth difference. The deviation distribution was highly nonuniform because the distance from the inner edge to the pitch circle was much smaller than the distance from the pitch circle to the outer edge. The resulting modification was too weak near the inner side and too strong near the outer side, which pushed the contact mark back toward the inner edge. For this small-ratio face gear, tooth-number-difference modification alone was therefore not sufficient. I decided to keep the shaper cutter tooth number equal to the pinion tooth number, \(z_s=z_2=40\), and to modify the pinion flanks directly. This gave me independent control over profile modification and lead modification while preserving the basic face gear conjugate geometry.
Tooth contact analysis of the initial face gear pair. I used the standard TCA condition for a face gear pair. In a fixed coordinate system, the position vectors and unit normal vectors of the pinion and face gear must coincide at the instantaneous contact point:
$$r_1^{(f)}(u_1,v_1,\phi_1)=r_2^{(f)}(u_2,v_2,\phi_2)$$
$$n_1^{(f)}(u_1,v_1,\phi_1)=n_2^{(f)}(u_2,v_2,\phi_2)$$
$$|n_1^{(f)}|=|n_2^{(f)}|=1$$
Here \(u_1,v_1\) are the surface coordinates of the pinion, \(u_2,v_2\) are the surface coordinates of the face gear, and \(\phi_1,\phi_2\) are the rotation angles. I solved these equations numerically for each pinion rotation increment. The transmission error was computed as
$$\Delta\phi_2(\phi_1)=\left[\phi_2(\phi_1)-\phi_2^{(0)}\right]-\frac{z_1}{z_2}\left[\phi_1-\phi_1^{(0)}\right]$$
For the initial unmodified or lightly modified face gear pair, the TCA contact path was approximately a parabolic curve opening toward the outer radius. The path covered a large part of the face width, but the contact points were concentrated toward the inner side. The transmission error amplitude was relatively large, about \(38\) angular units in the TCA output, and the curve did not alternate smoothly from tooth to tooth. A non-alternating transmission error curve is a warning sign for impact at engagement and for a reduced effective contact ratio. It also means that the face gear tooth tip may carry a disproportionate part of the load.
I represented the contact path on the face gear flank by a quadratic relation of the form
$$z_h(x_w)=z_{h0}+k_c\left(x_w-x_{w0}\right)^2$$
where \(z_h\) is the coordinate along the face width, \(x_w\) is the coordinate along the tooth height, and \(k_c\) controls the curvature of the path. For the initial design, \(k_c\) was large enough that the path moved quickly from the inner region toward the outer region, but the loaded contact still remained biased inward. The contact ratio estimated from the finite element sequence was about \(1.83\). This value is useful for a face gear pair, but it is not sufficient if the contact area is shifted toward one edge.
Loaded tooth contact analysis and stress screening. I built a five-tooth finite element model of the face gear pair and used the middle tooth as the main observation tooth. The contact problem was solved with a standard unilateral contact formulation:
$$[K]\{u\}=\{F\}$$
$$p_i\ge0,\qquad g_i\ge0,\qquad p_i g_i=0$$
$$F_c=\sum_{i=1}^{N}p_i A_i$$
Here \(p_i\) is the contact pressure at contact candidate \(i\), \(g_i\) is the gap, \(A_i\) is the associated area, and \(F_c\) is the total contact force. The maximum contact stress and maximum root bending stress were extracted from the loaded solution:
$$\sigma_H^{\max}=\max_{A_c}p(x,y)$$
$$\sigma_F^{\max}=\max_{\Gamma_f}\sigma_{\mathrm{vM}}$$
For the initial design, the maximum contact stress was about \(970\ \mathrm{MPa}\) on the pinion and \(975\ \mathrm{MPa}\) on the face gear. The maximum root bending stress was about \(371\ \mathrm{MPa}\) on the pinion and \(212\ \mathrm{MPa}\) on the face gear. These stresses are not necessarily outside the allowable range for the selected material, but the contact pattern was poor because the load was concentrated near the inner radius. I also observed the risk of edge contact near the outer tooth tip. To control this risk, I introduced a tooth-tip chamfer on the face gear. The final design parameters are listed in Table 4, and the initial pinion modification parameters are listed in Table 5.
Table 4. Final geometric design parameters of the face gear pair.
| Parameter | Value |
|---|---|
| Module \(m\) | 3.9 mm |
| Pinion teeth \(z_2\) | 40 |
| Shaper cutter teeth \(z_s\) | 40 |
| Face gear teeth \(z_1\) | 51 |
| Inner radius \(R_1\) | 97.5 mm |
| Outer radius \(R_2\) | 124.5 mm |
| Pressure angle \(\alpha\) | 25° |
| Outer chamfer length \(L\) | 16.3 mm |
| Outer chamfer height \(h\) | 3.12 mm |
| Face gear tooth-tip chamfer radius | 0.3 mm |
| Pinion tooth-tip chamfer radius | 0.5 mm |
The outer chamfer angle follows from the chamfer geometry as
$$\theta_c=\arctan\left(\frac{h}{L}\right)=\arctan\left(\frac{3.12}{16.3}\right)=10.83^\circ$$
This chamfer removes the sharply pointed outer corner of the face gear tooth and reduces the chance of edge contact when the contact path moves toward the outer radius. It also makes it possible to use a larger outer radius without violating the pointing condition.
Table 5. Initial pinion flank modification parameters for the face gear pair.
| Modification parameter | Initial value |
|---|---|
| Profile modification amplitude \(a_1\) | 3 μm |
| Profile modification amplitude \(a_2\) | 10 μm |
| Profile first transition \(h_1\) | 3.9 mm |
| Profile second transition \(h_2\) | 4.875 mm |
| Lead inner transition \(b_a\) | 9 mm |
| Lead outer transition \(b_b\) | 19 mm |
| Lead modification amplitude \(c_1\) | 20 μm |
| Lead modification amplitude \(c_2\) | 3 μm |
Parabolic modification model. I used parabolic modification curves because they are smooth and can be manufactured on a pinion by profile grinding or lead crowning. The total modification was the sum of a profile modification and a lead modification:
$$\delta(u,v)=\delta_p(u)+\delta_l(v)$$
The profile modification was defined piecewise as
$$\delta_p(u)=a_1\left(\frac{u}{h_1}\right)^2,\qquad 0\le u\le h_1$$
$$\delta_p(u)=a_1+(a_2-a_1)\left(\frac{u-h_1}{h_2-h_1}\right)^2,\qquad h_1<u\le
The lead modification was defined by two control distances \(b_a<b_b\):
$$\delta_l(v)=c_1\left(\frac{|v|}{b_a}\right)^2,\qquad |v|\le b_a$$
$$\delta_l(v)=c_1+(c_2-c_1)\left(\frac{|v|-b_a}{b_b-b_a}\right)^2,\qquad b_a<|v|\le b_b$$
In these equations, \(u\) is the coordinate along the tooth profile, \(v\) is the coordinate along the tooth lead, \(a_1,a_2\) are profile modification amplitudes, \(c_1,c_2\) are lead modification amplitudes, and \(h_1,h_2,b_a,b_b\) are transition positions. I selected the initial values in Table 5 after several trial TCA runs. The main purpose of the profile modification was to rotate the contact path on the face gear and avoid edge contact at the tooth tip. The main purpose of the lead modification was to concentrate the contact path near the middle of the face width and reduce the eccentric load toward the inner radius.
I also defined an optimization objective to rank candidate modifications. The objective included transmission error amplitude, contact-area ratio, maximum contact stress, and maximum root bending stress:
$$\min J=w_1\frac{\max|\Delta\phi_2|}{\Delta\phi_2^{\mathrm{ref}}}+w_2\frac{|\Delta R_c|}{R_c^{\mathrm{ref}}}+w_3\frac{\max\sigma_H}{\sigma_H^{\mathrm{allow}}}+w_4\frac{\max\sigma_F}{\sigma_F^{\mathrm{allow}}}$$
Here \(w_1,w_2,w_3,w_4\) are weights, \(\Delta R_c\) is the offset of the contact center from the desired mid-face position, and \(\sigma_H^{\mathrm{allow}},\sigma_F^{\mathrm{allow}}\) are allowable stresses. I required the contact path to remain inside the working flank and the loaded contact zone to avoid the chamfered tip and the root fillet. The best candidates were then checked with LTCA.
Installation error model. A face gear pair in an aeroengine central transmission is never perfectly aligned. I considered three independent installation errors: axial offset \(\Delta q\), shaft-angle error \(\Delta\gamma\), and axis-intersection error \(\Delta E\). I assembled a misalignment transformation matrix
$$M_m=M_q(\Delta q)M_\gamma(\Delta\gamma)M_E(\Delta E)$$
and transformed the pinion position and normal vectors into the face gear coordinate system:
$$r_2^{(f)}=M_m r_1^{(f)}$$
$$n_2^{(f)}=M_m n_1^{(f)}$$
The TCA equations then became
$$r_1^{(f)}(u_1,v_1,\phi_1)-r_2^{(f)}(u_2,v_2,\phi_2)=0$$
$$n_1^{(f)}(u_1,v_1,\phi_1)\times n_2^{(f)}(u_2,v_2,\phi_2)=0$$
I solved these equations for several error combinations. The error cases are listed in Table 6. For each case, I extracted the transmission error amplitude
$$\Delta\phi_2^{\mathrm{amp}}=\max\Delta\phi_2-\min\Delta\phi_2$$
and the contact path on the face gear. I then compared the results with the standard, error-free installation.
Table 6. Installation error cases used in the face gear TCA study.
| Case | Axial offset \(\Delta q\) (mm) | Shaft-angle error \(\Delta\gamma\) (°) | Axis-intersection error \(\Delta E\) (mm) |
|---|---|---|---|
| 1 | 0 | 0 | 0 |
| 2 | 0.025 | 0 | 0 |
| 3 | -0.050 | 0 | 0 |
| 4 | 0 | -0.005 | 0 |
| 5 | 0 | 0.015 | 0 |
| 6 | 0 | 0 | -0.030 |
| 7 | 0 | 0 | 0.050 |
| 8 | 0.025 | 0.005 | -0.030 |
| 9 | 0.025 | -0.005 | 0.030 |
The TCA results showed clear trends. The contact path was most sensitive to shaft-angle error \(\Delta\gamma\), next to axial offset \(\Delta q\), and least to axis-intersection error \(\Delta E\). I summarized this sensitivity by the derivatives
$$S_{\Delta q}=\frac{\partial\Delta\phi_2^{\mathrm{amp}}}{\partial\Delta q},\qquad S_{\Delta\gamma}=\frac{\partial\Delta\phi_2^{\mathrm{amp}}}{\partial\Delta\gamma},\qquad S_{\Delta E}=\frac{\partial\Delta\phi_2^{\mathrm{amp}}}{\partial\Delta E}$$
I found that
$$|S_{\Delta\gamma}|>|S_{\Delta q}|>|S_{\Delta E}|$$
For the contact path, I approximated the shift along the face width by a linear relation:
$$\Delta z_h=\alpha_q\Delta q+\alpha_\gamma\Delta\gamma+\alpha_E\Delta E$$
The signs of the coefficients are important. Positive axial offset or positive shaft-angle error moved the contact path toward the outer radius of the face gear. Negative axial offset or negative shaft-angle error moved the contact path toward the inner radius. Positive axis-intersection error moved the contact path toward the inner radius, while negative axis-intersection error moved it toward the outer radius. When the individual errors acted in the same direction, the total contact shift increased. When they acted in opposite directions, the total shift decreased. This means that installation errors can either add or cancel, and a tolerance allocation must consider the combined effect rather than each error separately.
I also examined the transmission error under installation errors. A negative axial offset and a positive shaft-angle error both reduced the transmission error amplitude for the present face gear pair. They made the transmission error curve smoother and more continuous. A positive axial offset and a negative shaft-angle error increased the transmission error amplitude and pushed the contact path toward the outer radius, which increased the risk of edge contact near the face gear tip. Axis-intersection error had a smaller effect on transmission error, but it still changed the contact position enough to matter for a high-power face gear pair.
Table 7. Qualitative influence of installation errors on the face gear pair.
| Error variable | Positive direction | Negative direction | Influence on transmission error |
|---|---|---|---|
| Axial offset \(\Delta q\) | Contact moves outward | Contact moves inward | Negative \(\Delta q\) improved smoothness |
| Shaft-angle error \(\Delta\gamma\) | Contact moves outward | Contact moves inward | Positive \(\Delta\gamma\) improved smoothness |
| Axis-intersection error \(\Delta E\) | Contact moves inward | Contact moves outward | Smaller effect than \(\Delta q\) and \(\Delta\gamma\) |
Refinement of the face gear pair modification. The initial modification improved the eccentric load, but the TCA results still showed that some cases had discontinuous transmission error. The contact path was distributed over a large part of the face width, but the transmission error curve did not alternate in a way that would guarantee smooth meshing. I therefore refined the lead modification parameters while keeping the profile modification unchanged. The original lead transitions were too far apart, which made the contact path narrow near the center and left the transition zones too steep. I reduced the outer lead transition and increased the inner lead transition so that the crowning was more gradual. The improved values are listed in Table 8.
Table 8. Improved lead modification parameters for the face gear pair.
| Modification parameter | Initial value | Improved value |
|---|---|---|
| Profile amplitude \(a_1\) | 3 μm | 3 μm |
| Profile amplitude \(a_2\) | 10 μm | 10 μm |
| Profile transition \(h_1\) | 3.9 mm | 3.9 mm |
| Profile transition \(h_2\) | 4.875 mm | 4.875 mm |
| Lead inner transition \(b_a\) | 9 mm | 12.4 mm |
| Lead outer transition \(b_b\) | 19 mm | 15.6 mm |
| Lead amplitude \(c_1\) | 20 μm | 20 μm |
| Lead amplitude \(c_2\) | 3 μm | 3 μm |
After this refinement, the transmission error curve became much more continuous. The amplitude dropped from the initial large value to approximately \(20\) angular units, and the curve had a smoother tooth-to-tooth transition. The contact path remained close to the middle of the face width and covered most of the working flank. The improved contact line was no longer concentrated at the inner radius, and the risk of edge contact at the outer tip was greatly reduced. This confirmed that the lead modification, not the profile modification alone, was the main control for the eccentric load in this small-ratio face gear pair.
Final LTCA results. I repeated the five-tooth loaded contact analysis with the improved modification. The maximum contact stress remained below the allowable value for the selected material. The final stress results are summarized in Table 9. The contact area reached about \(86.5\%\) of the working flank, and the contact ratio was about \(1.83\). The maximum contact stress was about \(970\ \mathrm{MPa}\) on the pinion and \(975\ \mathrm{MPa}\) on the face gear. The maximum root bending stress was about \(371\ \mathrm{MPa}\) on the pinion and \(212\ \mathrm{MPa}\) on the face gear. These values indicate that a high-power, small-ratio face gear pair can be designed within the given space if the flanks are modified properly.
Table 9. Final LTCA stress results for the face gear pair.
| Component | Maximum contact stress (MPa) | Maximum root bending stress (MPa) |
|---|---|---|
| Pinion | 970 | 371 |
| Face gear | 975 | 212 |
Discussion of the face gear design logic. The most important lesson I learned from this face gear study is that a small transmission ratio changes the relative position of the pitch circle and the mid-face-width. In a large-ratio face gear, the pitch region is often close to the center of the usable face width. In a small-ratio face gear, however, the pitch region is close to the inner radius, so an unmodified face gear pair tends to contact near the inner edge. If the designer applies only a tooth-number-difference modification, the modification amount is not symmetric with respect to the usable face width. The inner side receives too little modification and the outer side receives too much, which worsens the eccentric load. Direct pinion modification avoids this asymmetry because the profile and lead modifications can be independently tuned.
I also found that the face gear tooth-tip chamfer is essential. Without the chamfer, the outer tip of the face gear is vulnerable to edge contact when the contact path moves outward under positive axial offset or positive shaft-angle error. The chamfer removes the sharp corner and reduces the stress concentration. The chamfer angle I used was about \(10.83^\circ\), which was sufficient to protect the tip while preserving a large effective face width. The pinion tip chamfer also helped avoid concentrated contact at the pinion addendum.
For the transmission error, I concluded that a continuous and alternating curve is more important than a very small amplitude. A face gear pair with a small but discontinuous transmission error can still produce impact and noise because the mesh stiffness changes abruptly at tooth engagement. The improved lead modification made the transmission error curve continuous and reduced the amplitude to a level that is acceptable for a high-power face gear transmission. The contact path was also stable under the expected installation errors, especially when the errors were small and partially cancelling.
Installation tolerance recommendations for the face gear pair. Based on the TCA and LTCA results, I recommend that the shaft-angle error \(\Delta\gamma\) receive the tightest tolerance. The axial offset \(\Delta q\) should receive the next tightest tolerance. The axis-intersection error \(\Delta E\) can be slightly looser because its effect on the contact path and transmission error is smaller. If the assembly process can bias the axial offset slightly negative or the shaft-angle error slightly positive, the transmission error can be reduced for this particular face gear pair. However, such a bias must be verified experimentally because it also shifts the contact path. The combined error should be checked with the linear superposition relation
$$\Delta z_h=\alpha_q\Delta q+\alpha_\gamma\Delta\gamma+\alpha_E\Delta E$$
and with the transmission error amplitude
$$\Delta\phi_2^{\mathrm{amp}}=f(\Delta q,\Delta\gamma,\Delta E)$$
I would not rely on a single error value. Instead, I would define a tolerance box and evaluate its corner combinations. In this way, the face gear pair can be designed so that even the worst combination keeps the contact path inside the working flank and keeps the transmission error continuous.
Design equations I used for the final face gear pair. For clarity, I summarize the main equations that governed the final face gear design. The nominal ratio is
$$i=\frac{z_2}{z_1}$$
The pinion tip diameter constraint is
$$m(z_2+2)\le167\ \mathrm{mm}$$
The face gear inner and outer radius constraints are
$$R_{\min}\ge R_{\mathrm{undercut}},\qquad R_{\max}\le R_{\mathrm{pointed}}$$
The face gear pressure angle at an arbitrary radius is approximated by
$$\cos\alpha(d)=\frac{m_n z_n\cos\alpha_n}{d}$$
The total torque used in LTCA is
$$T=K_A K_v T_1$$
The total flank modification is
$$\delta(u,v)=\delta_p(u)+\delta_l(v)$$
The profile modification is
$$\delta_p(u)=a_1\left(\frac{u}{h_1}\right)^2,\qquad 0\le u\le h_1$$
$$\delta_p(u)=a_1+(a_2-a_1)\left(\frac{u-h_1}{h_2-h_1}\right)^2,\qquad h_1<u\le
The lead modification is
$$\delta_l(v)=c_1\left(\frac{|v|}{b_a}\right)^2,\qquad |v|\le b_a$$
$$\delta_l(v)=c_1+(c_2-c_1)\left(\frac{|v|-b_a}{b_b-b_a}\right)^2,\qquad b_a<|v|\le b_b$$
The TCA contact condition is
$$r_1^{(f)}=r_2^{(f)},\qquad n_1^{(f)}=n_2^{(f)}$$
The transmission error is
$$\Delta\phi_2(\phi_1)=\left[\phi_2(\phi_1)-\phi_2^{(0)}\right]-\frac{z_1}{z_2}\left[\phi_1-\phi_1^{(0)}\right]$$
The loaded contact equilibrium is
$$[K]\{u\}=\{F\}$$
$$p_i\ge0,\qquad g_i\ge0,\qquad p_i g_i=0$$
The installation error transformation is
$$M_m=M_q(\Delta q)M_\gamma(\Delta\gamma)M_E(\Delta E)$$
These equations formed a consistent framework for designing and evaluating the high-power, small-ratio spur face gear pair.
Final assessment. The final face gear pair satisfied the space limitation, the torque requirement, and the contact stress requirement. The pinion had 40 teeth, the face gear had 51 teeth, and the module was 3.9 mm. The face gear inner radius was 97.5 mm and the outer radius was 124.5 mm. A large outer chamfer with a height of 3.12 mm and a length of 16.3 mm prevented tooth pointing and edge contact. The pinion was modified in both the profile and lead directions. The profile modification rotated the contact path away from the face gear tip, and the lead modification moved the contact toward the middle of the face width. The improved lead transitions were 12.4 mm and 15.6 mm. The final contact area was about 86.5% of the working flank, and the contact ratio was about 1.83. The transmission error became continuous, and the maximum stresses remained acceptable.
I conclude that a high-power, small-transmission-ratio spur face gear pair can be designed within a tight space if the designer treats the face gear as a system problem. The geometry, the shaper cutter tooth number, the pinion modification, the tooth-tip chamfer, and the installation tolerances must all be considered together. A face gear pair with a small ratio is especially sensitive to axial offset and shaft-angle error, so the assembly tolerances should be assigned with care. When these factors are controlled, the face gear pair can provide a compact, strong, and smooth transmission for a high-power application.
</b_b\):