Remanufactured Double Circular Arc Gear Tooth Surface Cutting

I began this research because double circular arc gears are widely used in pumping unit reducers, where they must carry heavy loads and maintain reliable transmission during the lifting process. In many onshore oilfields, pumping units remain the main lifting equipment, and a large number of units are still in service. When a double circular arc gear fails, the failure is often limited to a few damaged teeth, yet the entire gear may be scrapped. I saw a strong economic and environmental reason to develop a remanufacturing method that can restore only the damaged teeth instead of replacing the whole gear. My work therefore concentrates on parameter measurement, single-tooth gear cutting, forming principles, disc hob design, simulation, machine tool layout, and error control. The phrase gear cutting appears throughout this study because the central technical challenge is to achieve accurate and efficient gear cutting on a remanufactured double circular arc gear.

I first reviewed the difference between involute gears and circular arc gears. Involute gears are easy to manufacture and measure, and they allow center distance variation, but their contact stress and bending strength are not always sufficient for heavy-duty reducers. Circular arc gears use a point-meshing system, and their normal tooth profile is an arc. A single circular arc gear has only one convex or concave arc on each tooth flank, while a double circular arc gear has both convex and concave arcs. The double circular arc gear is more widely used because it offers higher bending strength, higher contact strength, and stronger load capacity. These advantages make it suitable for pumping unit reducers. However, the same geometric features that improve load capacity also make measurement, gear cutting, and repair more difficult.

My research objective was to establish a complete method for remanufacturing a damaged double circular arc gear by cutting only the missing or damaged teeth. The method includes four main parts. First, I measured the unknown original parameters of the gear. Second, I derived the forming principle for single-tooth generation. Third, I designed a disc hob and simulated the gear cutting process. Fourth, I designed the machine tool layout and analyzed the axial pitch error and tooth end relief. In this way, I connected measurement, theory, tool design, simulation, and error compensation into one workflow.

Parameter Determination for Remanufactured Double Circular Arc Gears

For a double circular arc gear whose original design parameters are unknown, the first problem is to determine the normal module, helix angle, number of teeth, and face width. The number of teeth and face width can usually be measured directly. The normal module and helix angle are more difficult. The normal module is important because almost all other tooth profile parameters can be derived from it. The helix angle is important because the actual tooth surface is a helicoid, and gear cutting must follow the correct helix. I therefore developed a measurement method that combines laser scanning with reverse engineering data processing.

The basic tooth profile of a double circular arc gear is standardized. The full depth is twice the normal module, the addendum is nine tenths of the normal module, and the dedendum is eleven tenths of the normal module. The convex arc radius, concave arc radius, root arc radius, and transition arc radius are all proportional to the normal module. Table 1 summarizes the main basic rack parameters for several module ranges.

Parameter Symbol or relation Value or range
Normal module m 1.5 to 50 mm
Pressure angle alpha 24 degrees
Full depth h 2m
Addendum h_a 0.9m
Dedendum h_f 1.1m
Convex arc radius rho_a 1.3m
Concave arc radius rho_f 1.42m to 1.34m depending on module
Convex center offset N_a 0.6289m
Concave center offset N_f 0.7086m to 0.6455m depending on module
Root arc radius r_root 0.4030m to 0.3520m
Transition arc radius r_trans 0.5049m to 0.4858m

I used a handheld 3D laser scanner because it can capture a large amount of surface data without contact. The scanner works on the triangulation principle. A laser emitter projects a beam onto the gear surface, and a camera receives the reflected beam. The spatial coordinates are computed from the triangle formed by the emitter, the camera, and the point on the surface. I set the scanning resolution to 0.2 mm because the teeth are relatively small and the measurement must capture the addendum and dedendum circles accurately.

Before scanning, I cleaned the gear surface to remove dust and oil. I then placed positioning markers on the gear shaft. The markers must be dense enough for reliable registration but not so dense that the data become unnecessarily large. I avoided placing markers on sharp edges, small features, and highly curved areas. After marker placement, I scanned the gear from multiple angles. I first scanned the low-curvature regions and then the tooth flanks. I maintained a nearly constant distance between the scanner and the surface to improve accuracy. The scanned data were stored as a triangular mesh.

I imported the mesh into reverse engineering software for data processing. First, I created surface regions and fitted the cylindrical surfaces that represent the gear shaft. From these fitted surfaces, I established the gear axis. I then created two perpendicular planes on the axis and aligned the model coordinate system. Next, I removed redundant triangles, repaired non-manifold edges, filled holes, and deleted overlapping faces. After these operations, the model was clean enough for measurement.

I created a series of section planes perpendicular to the gear axis at intervals of 10 mm. In each section, I generated a sketch of the tooth profile. I then fitted the addendum circle and the dedendum circle using a three-point circle command. The difference between the addendum radius and the dedendum radius gives half of the full depth. Because the full depth is equal to twice the normal module, I could calculate the normal module. The dedendum height is equal to 1.1 times the normal module, so the pitch circle diameter can be found from the root circle diameter. Finally, the helix angle can be calculated from the pitch circle diameter, the number of teeth, and the normal module. The governing equations are:

$$
h = \frac{d_a – d_f}{2}
$$

$$
h = 2m
$$

$$
d_f = d – 2h_f = d – 2.2m
$$

$$
d = \frac{mz}{\cos\beta}
$$

Table 2 lists the measured addendum and dedendum radii from several sections. The values are close to each other, which confirms that the measurement is stable.

Section Addendum radius (mm) Dedendum radius (mm)
1 60.3336 51.5069
2 60.3827 51.4943
3 60.3528 51.5245
4 60.3453 51.5357
5 60.4027 51.5326
6 60.3633 51.5643
7 60.3830 51.5532

The average addendum radius was 60.3662 mm, and the average dedendum radius was 51.5302 mm. Therefore, the average full depth was 8.836 mm. The calculated normal module was 4.418 mm. Since standard modules are integers or simple decimals, I rounded the normal module to 4.5 mm. Using the dedendum height relation, the average dedendum height became 4.95 mm, and the average pitch circle diameter became 112.9604 mm. With 23 teeth and a normal module of 4.5 mm, the average helix angle was 23.61612 degrees. The original design helix angle was 23.4117 degrees. The measurement error was about 0.87 percent, which is small enough for the subsequent gear cutting operation.

Conjugate Principle and Tooth Surface Formation

To perform accurate gear cutting on a remanufactured double circular arc gear, I studied the conjugate principle of the gear pair. A double circular arc gear can be formed by a rack cutter whose normal profile consists of convex and concave arcs. The rack profile is symmetric about the pitch line. I defined a coordinate system fixed to the rack. The rack profile equations can be written in a unified form as:

$$
\begin{cases}
X_f = N \mp \rho \cos\alpha \\
Y_f = u \\
Z_f = e – \rho \sin\alpha
\end{cases}
$$

Here, alpha is the pressure angle, rho is the arc radius, e is the offset of the arc center from the pitch line, N is the shift of the arc center from the tooth symmetry line, and u is the displacement along the tooth width direction. The double signs represent the left and right flanks. For the convex tooth, the pressure angle is positive. For the concave tooth, the pressure angle is negative. The offset e is positive when the arc center lies outside the pitch cylinder and negative when it lies inside. The shift N is positive when the arc center and the arc are on opposite sides of the symmetry line, and negative when they are on the same side.

I then transformed the rack profile into a coordinate system whose axis is parallel to the gear axis. The transformation is:

$$
\begin{cases}
X_d = X_f \cos\beta + Y_f \sin\beta \\
Y_d = -X_f \sin\beta + Y_f \cos\beta \\
Z_d = Z_f
\end{cases}
$$

Substituting the rack equations gives the double circular arc rack forming surface in the new coordinate system:

$$
\begin{cases}
X_d = (N \mp \rho \cos\alpha)\cos\beta + u \sin\beta \\
Y_d = -(N \mp \rho \cos\alpha)\sin\beta + u \cos\beta \\
Z_d = e – \rho \sin\alpha
\end{cases}
$$

To find the conjugate contact condition, I used the kinematic method. The condition is that the relative velocity at the contact point must be perpendicular to the common normal. In equation form:

$$
\mathbf{n} \cdot \mathbf{v} = 0
$$

The normal vector is obtained by taking the cross product of the two tangent vectors of the rack surface. The result is:

$$
\begin{cases}
n_x = \cos\beta \cos\alpha \\
n_y = -\sin\beta \cos\alpha \\
n_z = \mp \sin\alpha
\end{cases}
$$

Using the instantaneous rotation method for single-tooth generation, I derived the relative velocity at the contact point. The contact condition becomes:

$$
r_1 \cot\beta – N + e \cot\alpha \mp u \sin\beta = 0
$$

This equation is the conjugate contact condition for the remanufactured double circular arc gear. By combining the rack surface equations with this condition, I obtained the tooth surface equations of the double circular arc gear. The final form is:

$$
\begin{cases}
X_1 = ( \rho \sin\alpha + e + r_1 ) \sin\phi + ( \rho \cos\alpha + e \cot\alpha ) \cos\beta \cos\phi \\
Y_1 = r_1 \phi \cot\beta – \left( \rho \cos\alpha \sin\beta – e \cot\alpha \cos\beta \cot\beta – \frac{N}{\sin\beta} \right) \\
Z_1 = ( \rho \sin\alpha + e + r_1 ) \cos\phi – ( \rho \cos\alpha + e \cot\alpha ) \cos\beta \sin\phi
\end{cases}
$$

I also derived the meshing surface equations for two auxiliary racks and the gear. After eliminating the rack parameters, the meshing surface equations take the form:

$$
\left( \frac{Z_f}{e} \right)^2 + \left[ \frac{(X_f + Z_f \cos\beta)^2 + Y_f^2}{\rho_m^2} \right] \tan^2\beta = 1
$$

For two gears with crossed axes, the meshing line is the intersection of the two meshing surfaces. Solving the two equations gives the meshing line parameter equations:

$$
\begin{cases}
X_f = \mp ( \rho_m \cos\alpha_m + e_m \cot\alpha_m ) \\
Y_f = 0 \\
Z_f = \rho_m \sin\alpha_m + e_m
\end{cases}
$$

When the arc center lies on the pitch line, the offset e is zero, and the meshing line becomes a circular arc in the normal plane. This result proves that the instantaneous contact line during gear cutting is a normal circular arc. Therefore, single-tooth generation is theoretically feasible for remanufactured double circular arc gears.

Single-Tooth Generative Gear Cutting Method

In conventional hobbing of a double circular arc gear, the gear cutting process first generates the tooth profile along the tooth height direction and then feeds along the helix direction. The entire gear is cut tooth by tooth in a continuous indexing motion. This method is efficient for new gears but not for remanufacturing, because only a few teeth may be damaged. If the whole gear is hobbed again, the good teeth are also recut, which wastes time and may remove the hardened layer. I therefore proposed a single-tooth generative method that reverses the order of the spiral motion and the generating motion. In this method, the gear cutting tool first moves along the helix direction to cut the tooth width, and then the generating motion is performed to form the tooth profile. The process is discontinuous because the gear surface is a helicoid and cannot be generated by a simple reversible motion. The workpiece is indexed after each tooth is completed.

The single-tooth generative method is based on the same conjugate principle as hobbing, but the motion sequence is changed. The cutting motion consists of four parts: cutter rotation, spiral feed, generating feed, and workpiece rotation. I designed the transmission scheme for a dedicated machine tool. The cutter rotation chain drives the disc hob. The spiral feed chain moves the cutter carriage along the gear axis. The generating feed chain moves the cutter carriage perpendicular to the gear axis. The workpiece rotation chain rotates the gear blank. The spiral feed and workpiece rotation are synchronized by a CNC controller to produce the correct helix angle. The generating feed and workpiece rotation are synchronized to produce the correct tooth profile.

The transmission principle can be summarized by the following relations. For the spiral motion, the axial displacement and the workpiece rotation must satisfy:

$$
\tan\beta = \frac{R \theta}{b}
$$

where R is the pitch radius, theta is the workpiece rotation angle, and b is the axial displacement. For the generating motion, the cutter moves as a rack relative to the gear. The generating feed speed is related to the workpiece rotation speed by:

$$
v_g = \frac{\pi d n_w}{60000}
$$

where v_g is the generating feed speed in m/s, d is the workpiece diameter in mm, and n_w is the workpiece speed in rpm. These relations were used to determine the motor speeds and gear ratios in the machine tool design.

Disc Hob Design for Single-Tooth Gear Cutting

For single-tooth gear cutting, I designed a disc hob whose profile is the same as a standard double circular arc hob for the same module. The normal module of the target gear is 4.5 mm. According to the standard hob profile, the hob has a convex working section, a transition section, a concave working section, and a non-working top section. Table 3 lists the hob profile dimensions for module 4.5 mm.

Section x coordinate (mm) y coordinate (mm)
Top non-working start 0.000 0.000
Convex working start 0.502 1.249
Transition start 4.050 3.117
Concave working start 5.669 4.089
Convex working end 0.109 0.617
Transition end 1.348 1.987
Concave working end 4.288 3.409
Outer point 6.537 4.252

The outer diameter of the disc hob was selected as 112 mm, which matches the standard hob outer diameter for module 4.5 mm. The hob material is high-speed steel. The disc shape allows the hob to be used in a single-tooth gear cutting operation where the tool must move along the helix first and then generate the profile.

I simulated the gear cutting process in MATLAB to verify the single-tooth generative method. The simulation was performed in three stages. First, I constructed the planar hob profile using the three-point circle principle. For any three points on an arc, the circle center and radius can be found by solving the perpendicular bisector equations. The determinant form is:

$$
\begin{vmatrix}
x^2 + y^2 & x & y & 1 \\
x_1^2 + y_1^2 & x_1 & y_1 & 1 \\
x_2^2 + y_2^2 & x_2 & y_2 & 1 \\
x_3^2 + y_3^2 & x_3 & y_3 & 1
\end{vmatrix} = 0
$$

Using this principle, I generated the eight arc segments that form the double circular arc hob profile. Then I simulated the planar generative motion. In each step, the hob profile was translated by a small distance and rotated by a small angle. The envelope of the successive positions formed the gear tooth profile. This is the same as the rack generating motion in gear cutting.

Next, I extended the simulation to three dimensions. The spatial hob profile was obtained by adding the helix angle to the planar profile. The coordinate transformation is:

$$
\begin{cases}
x_3 = x_2 \\
y_3 = x_2 \tan\beta \\
z_3 = y_2
\end{cases}
$$

The helix path of the gear tooth was derived from the tooth surface equation. For a constant pressure angle, the helix equation is:

$$
\begin{cases}
X = ( \rho \sin\alpha + e + r ) \sin\phi – ( \rho \cos\alpha + e \cot\alpha ) \cos\beta \cos\phi \\
Y = r \phi \cot\beta – \left( \rho \cos\alpha \sin\beta – e \cot\alpha \cos\beta \cot\beta – \frac{N}{\sin\beta} \right) \\
Z = ( \rho \sin\alpha + e + r ) \cos\phi + ( \rho \cos\alpha + e \cot\alpha ) \cos\beta \sin\phi
\end{cases}
$$

I then translated the spatial hob profile along this helix. Finally, I combined the spiral translation with the planar generating motion to obtain the three-dimensional envelope of the single tooth. The simulation showed that the disc hob can generate the correct double circular arc tooth surface when the spiral motion and generating motion are applied in the proposed sequence. This confirmed that the single-tooth generative gear cutting method is feasible.

Machine Tool Layout and Motion Design

I designed the layout of a dedicated machine tool for single-tooth gear cutting of remanufactured double circular arc gears. The machine tool has a base, a generating feed motor, a rotary support, a cutter rotation motor, a disc hob, a workpiece fixture, a workpiece rotation motor, and a spiral feed motor. The cutter rotation motor drives the disc hob through a belt or gear train. The spiral feed motor drives a lead screw that moves the cutter carriage along the gear axis. The generating feed motor drives another lead screw that moves the cutter carriage perpendicular to the gear axis. The workpiece rotation motor drives the workpiece through a worm gear and a reduction gearbox. The rotary support carries the cutter carriage and allows the cutter to be oriented at the helix angle.

The transmission system has four main chains and three CNC synchronization links. The cutter rotation chain is independent and is controlled by a variable-frequency motor. The spiral feed chain and the workpiece rotation chain are synchronized by the CNC controller to produce the helix. The generating feed chain and the workpiece rotation chain are synchronized to produce the tooth profile. The synchronization equations are:

$$
n_w = \frac{v_s \sin\beta}{2\pi R}
$$

$$
n_g = \frac{v_g}{p_h}
$$

where n_w is the workpiece speed, v_s is the spiral feed speed, beta is the helix angle, R is the pitch radius, n_g is the generating motor speed, v_g is the generating feed speed, and p_h is the lead screw pitch. These equations were used to set the gear ratios and motor speeds.

I calculated the cutting parameters for a typical remanufactured double circular arc gear. The radial cutting depth was 0.5 mm per revolution. The cutting speed was calculated from the standard cutting speed formula:

$$
v_0 = \frac{C_v}{T^m f^{y_v} m^{x_v}} k_v
$$

For gray cast iron and a module of 4.5 mm, the cutting speed was 36.9486 m/min. The hob speed was:

$$
n = \frac{1000 v_0}{\pi d_0}
$$

where d_0 is the hob outer diameter. With d_0 equal to 112 mm, the hob speed was 105.00993 rpm. The cutting power was estimated by:

$$
P_c = \frac{C_{Pc} f^{y_{Pc}} m^{x_{Pc}} d_0^{u_{Pc}} v_0}{10^5} k_{Pc}
$$

The cutting power was 0.214875 kW. The power required to drive the hob and the arbor was 0.00220 kW. The maximum cutting force was calculated from an empirical formula for gear hobbing. The maximum force was 0.9331 kN, which produced a torque of 56.2193 N m. A reduction gearbox with a ratio of 26 was used so that the motor only needed to provide 2.162 N m. The selected cutter motor therefore had a power greater than 0.246 kW and a rated torque greater than 2.162 N m.

The spiral feed speed was set to 2.15544 m/min. The lead screw pitch was 2.5 mm, so the spiral feed motor speed was 63.86025 rpm. A reduction gearbox with a ratio of 25 was used. The required motor torque was 4.5 N m at a speed of 1596.5062 rpm. The workpiece rotation speed was 2.921614 rpm. A reduction gearbox with a ratio of 7.2 was used to reduce the axial pitch error. The workpiece motor needed to provide 0.9 N m at 610.0322 rpm. The generating feed speed was 0.0171303 m/s. The generating lead screw pitch was 2.5 mm, so the generating motor speed was 25.6875 rpm. A reduction gearbox with a ratio of 25 was used. The required motor torque was 3.5 N m at 667.875 rpm. Table 4 summarizes the main motion parameters.

Motion Speed or feed Reduction ratio Required motor torque
Cutter rotation 105.00993 rpm 26 2.162 N m
Spiral feed 2.15544 m/min 25 4.5 N m
Workpiece rotation 2.921614 rpm 7.2 0.9 N m
Generating feed 0.0171303 m/s 25 3.5 N m

Axial Pitch Deviation in Single-Tooth Gear Cutting

Axial pitch deviation is one of the most important errors in double circular arc gears because it directly affects the smoothness of meshing and the transmission accuracy. The standard defines axial pitch deviation as the difference between the actual distance and the nominal distance between two adjacent same-side tooth flanks along a line parallel to the gear axis, measured in the normal direction. I analyzed how the step angles of the stepper motors affect the axial pitch deviation.

The workpiece rotation stepper motor has a step angle of 0.6 degrees. The spiral feed stepper motor has a step angle of 1.8 degrees. For one step of the workpiece motor, the workpiece rotates by 0.020691 degrees when the reduction ratio is 1. The spiral feed motor moves the cutter by 0.001999 mm per step. The theoretical helix angle is 23.4117 degrees. The number of spiral feed steps required for one workpiece step is:

$$
a = \frac{\theta_1 R}{s_2}
$$

where theta_1 is the workpiece rotation angle, R is the pitch radius, and s_2 is the axial displacement per spiral step. The calculation gave 14.3967 steps. Since the number of steps must be an integer, I used 14 steps. The actual helix angle then became 24.0011 degrees. The axial pitch deviation before compensation was:

$$
F_{px}’ = \tan\beta_1 b – \tan\beta_2 b
$$

With a face width of 80 mm, the deviation was 40.85 micrometers. The standard tolerance for an 8-grade double circular arc gear with an effective face width of 80 mm is 25 micrometers. The deviation exceeded the tolerance. I therefore introduced a reduction gearbox with a ratio of 7.2 on the workpiece rotation motor. The workpiece rotation per step then became 0.00287 degrees. The number of spiral steps required for one workpiece step became 1.9995, which was rounded to 2. The actual helix angle became 23.3881 degrees. The axial pitch deviation was reduced to 15.51 micrometers, which is within the 25 micrometer tolerance. Table 5 lists the standard axial pitch tolerances.

Effective face width (mm) Grade 4 (um) Grade 5 (um) Grade 6 (um) Grade 7 (um) Grade 8 (um)
Up to 40 5.5 7 9 11 18
40 to 100 8 10 12 16 25
100 to 160 10 12 16 20 32
160 to 250 12 16 19 24 38
250 to 400 14 18 24 28 45
400 to 630 17 22 28 34 55

Tooth End Relief for Error Reduction

Even after the reduction gearbox was introduced, the remanufactured gear still experiences elastic deformation, bending and torsion deformation, and manufacturing errors. These effects can cause impact at the beginning and end of meshing. Tooth end relief is a practical way to reduce this impact. The principle is to remove a small amount of material from the tooth ends so that the tooth does not contact prematurely. The relief amount is the sum of three components: the elastic deformation of the tooth, the bending and torsion deformation of the gear body, and the machining error.

The elastic deformation component includes the normal bending deformation and the contact deformation. The normal bending deformation at one axial pitch from the tooth end is:

$$
\delta_f = (0.355 \times 10^{-9} P m + 0.3489 \times 10^{-7} m^2 + 0.7761 \times 10^{-5} m – 0.5018 \times 10^{-3}) \beta^2
$$

The contact deformation is:

$$
\delta_g = 0.423532 \left( \frac{K_j N}{\epsilon_{d\max} n_n d \cos\beta} \right)^{2/3} \left( \frac{A+B}{\lambda} \right)^{2/3}
$$

where K_j is the load factor, N is the transmitted power, epsilon_dmax is the maximum number of meshing points, n_n is the gear speed, d is the pitch diameter, and lambda is a coefficient depending on the curvature. The meshing point load is:

$$
P = \frac{2.0897 \times 10^7 K_j N}{\epsilon_{d\max} d n_n \cos\beta}
$$

For the target gear, the axial pitch was 35.5799 mm, and the distance between two meshing points on one tooth was 28.1491 mm. The gear had a face width of 80 mm, so the number of axial pitches was 2. The maximum number of meshing points was 6. The load factor was 2.72025. The transmitted power was 52.8 kW, the speed was 603.74 rpm, and the pitch diameter was 112.7852 mm. The meshing point load was 8005.4394 N. The normal bending deformation was 0.0252 mm. The contact deformation was 0.02176 mm. Therefore, the elastic deformation component was 0.04696 mm.

The bending and torsion deformation component is caused by the torque and the radial force. The torsion deformation of the gear body is:

$$
\Delta’ = \frac{K_r}{E} \left( \frac{w_i}{b} \right) \left( \frac{b}{d} \right)^2 \left( \frac{1}{1-K_i} \right) \left( a + c + \frac{a^2}{b} \right)
$$

The bending deformation is:

$$
\Delta” = \frac{1}{G} \left( \frac{w_i}{b} \right) \left( \frac{b}{d} \right)^2 \left( \frac{1}{1-K_i} \right)^4
$$

For the target gear, the torsion deformation was 0.09147 mm, and the bending deformation was 0.0049 mm. The total bending and torsion deformation was 0.09637 mm. The resulting change in helix angle was 0.0012 degrees. The axial pitch error caused by this deformation was 0.001721 mm. The corresponding relief component was:

$$
c_2 = \Delta p_x \sin\beta
$$

This gave 0.006838 mm. The machining error component was taken as the axial pitch tolerance, which was 0.016 mm. The total tooth end relief amount was:

$$
c = c_1 + c_2 + c_3 = 0.04696 + 0.006838 + 0.016 = 0.0697 \text{ mm}
$$

The relief length depends on the contact ratio. The contact ratio is:

$$
\epsilon_c = \frac{b’}{p_x}
$$

With a single-side face width of 80 mm and an axial pitch of 35.5799 mm, the contact ratio was 2.2486. The integer part was 2. The relief length for one end of the working region must satisfy:

$$
L_x \le \frac{b’}{\sin\beta} – \frac{\pi m \epsilon_p}{\sin\beta}
$$

The relief length for both ends must satisfy:

$$
L_{x2} \le \frac{b’}{2\sin\beta} – \frac{\pi m \epsilon_p}{2\sin\beta}
$$

For the target gear, the one-end relief length was less than or equal to 8.8401 mm, and the two-end relief length was less than or equal to 4.42 mm. The ideal relief curve is a hyperbola, but for ease of manufacturing, a circular arc can be used. The radius of the relief arc is:

$$
R_y \approx \frac{L_x^2}{2c}
$$

Using the calculated relief amount and length, the relief arc radius can be determined. Table 6 summarizes the error and relief parameters.

Parameter Value
Axial pitch 35.5799 mm
Distance between two meshing points 28.1491 mm
Normal bending deformation 0.0252 mm
Contact deformation 0.02176 mm
Elastic deformation relief component 0.04696 mm
Torsion deformation 0.09147 mm
Bending deformation 0.0049 mm
Total bending and torsion deformation 0.09637 mm
Axial pitch error from deformation 0.001721 mm
Bending and torsion relief component 0.006838 mm
Machining error relief component 0.016 mm
Total tooth end relief 0.0697 mm
One-end relief length limit 8.8401 mm
Two-end relief length limit 4.42 mm

Discussion and Practical Implications

The proposed method integrates measurement, forming theory, tool design, simulation, machine tool layout, and error compensation. For remanufacturing, the most important advantage is that only the damaged teeth need to be cut. This reduces machining time and preserves the undamaged teeth. The single-tooth generative gear cutting method is especially suitable for large gears, such as those used in pumping unit reducers, because the gear is difficult to remove and transport. By using a disc hob and a dedicated machine tool, the damaged tooth can be restored in place or with minimal disassembly.

The laser scanning measurement method is also practical. It does not require a coordinate measuring machine with a large working volume. The handheld scanner can be brought to the gear, and the reverse engineering software can process the data quickly. The measurement error of less than one percent is acceptable for determining the normal module and helix angle. The rounded module and calculated helix angle can then be used to generate the tool path and the hob profile.

The simulation in MATLAB confirmed that the disc hob can generate the correct tooth surface when the spiral motion and generating motion are applied in the proposed order. The simulation also helped verify the coordinate transformations and the contact condition. The machine tool layout and motor selection showed that the required motions can be achieved with standard stepper motors and reduction gearboxes. The axial pitch error analysis showed that a reduction gearbox on the workpiece rotation motor can reduce the error from 40.85 micrometers to 15.51 micrometers, which is within the 25 micrometer tolerance for an 8-grade gear. Tooth end relief further reduces the impact at meshing entry and exit.

In future work, I plan to build a prototype of the single-tooth gear cutting machine and conduct experiments on actual remanufactured double circular arc gears. I will measure the tooth surface after gear cutting and compare it with the theoretical surface. I will also test the transmission performance of the remanufactured gear pair and refine the tooth end relief curve. The results of this research can be extended to other types of circular arc gears and to the remanufacturing of large gears in other industrial applications.

Conclusion

I developed a complete method for the remanufactured double circular arc gear tooth surface cutting. The main conclusions are as follows. First, the normal module and helix angle of an unknown double circular arc gear can be determined by handheld laser scanning and reverse engineering data processing. The full depth is twice the normal module, and the helix angle can be calculated from the pitch diameter. For the target gear, the measured normal module was 4.5 mm, and the measured helix angle was 23.61612 degrees, with an error of 0.87 percent compared with the original design value. Second, the conjugate contact condition and tooth surface equations were derived for the double circular arc gear. The meshing line was shown to be a normal circular arc when the arc center lies on the pitch line. This provided the theoretical basis for single-tooth generative gear cutting. Third, a single-tooth generative method was proposed by reversing the order of the spiral motion and the generating motion. A disc hob with the standard double circular arc profile was designed, and MATLAB simulation verified that the disc hob can generate the correct tooth surface. Fourth, a dedicated machine tool layout was designed with four motion chains and three CNC synchronization links. The cutting parameters, motor speeds, and reduction ratios were calculated. Fifth, the axial pitch error was analyzed, and a reduction gearbox was used to reduce the error to within the standard tolerance. Tooth end relief was calculated, and the total relief amount was 0.0697 mm, with a one-end relief length of less than 8.8401 mm and a two-end relief length of less than 4.42 mm. The relief curve can be approximated by a circular arc. The proposed method provides a practical way to perform gear cutting on remanufactured double circular arc gears and can reduce cost, save material, and support green manufacturing.

Scroll to Top