Abstract:
This paper presents a comprehensive study on the determination of allowable assembly errors in helical gears of heavy truck transmissions using finite element simulation. The focus is on analyzing the mechanical behavior of helical gears under various assembly errors, specifically two-axis non-parallelism and tooth side clearance. The study aims to provide a theoretical basis for controlling the assembly process of heavy truck transmissions, thus enhancing their reliability and durability. By constructing 3D models of helical gear pairs and performing both static and dynamic finite element analyses, the paper quantifies the impact of assembly errors on contact stresses and dynamics, ultimately leading to the derivation of permissible limits for these errors. The results offer practical guidelines for engineers involved in the assembly of heavy truck transmissions.

Keywords: Heavy truck, helical gear, finite element analysis, two-axis non-parallelism, tooth side clearance, contact stress, dynamic simulation
1. Introduction
Heavy trucks play a crucial role in modern transportation systems, especially in the logistics and freight industry. The transmission system, as the heart of a heavy truck, significantly impacts its overall performance, efficiency, and reliability. Among the various components within the transmission, helical gears are widely used due to their smooth transmission, high load-bearing capacity, and reduced noise levels. However, assembly errors can significantly affect the performance of these gears, leading to premature failures such as tooth root cracks and breakages.
Traditional methods for determining assembly errors rely heavily on engineering experience, which lacks a scientific basis. To address this issue, this paper employs finite element simulation to investigate the effects of two common assembly errors—two-axis non-parallelism and tooth side clearance—on the mechanical behavior of helical gears. The results provide quantitative limits for these errors, guiding engineers in the assembly process to ensure optimal transmission performance.
2. Modeling and Simulation Methodology
2.1 Geometric Modeling
The helical gear models used in this study were created using Pro/ENGINEER, a popular 3D CAD software. The specific parameters of the helical gear pair, as shown in Table 1, were chosen to represent a typical application in heavy truck transmissions.
Table 1. Parameters of the Helical Gear Pair
| Parameter | Active Gear | Driven Gear |
|---|---|---|
| Number of Teeth | 14 | 35 |
| Pressure Angle | 20° | 20° |
| Module | 5 mm | 5 mm |
| Face Width | 20 mm | 20 mm |
| Helix Angle | 15° | 15° |
Based on these parameters, the 3D models of the helical gear pair were constructed and meshed for subsequent finite element analyses.
2.2 Finite Element Modeling
The finite element models were developed using ANSYS, a leading finite element analysis software. Static and dynamic simulations were performed to analyze the contact stress and dynamic behavior of the helical gear pair under different assembly error conditions.
2.2.1 Contact Pair Definition
Contact pairs were defined between the teeth of the active and driven gears to simulate their meshing behavior. A friction coefficient of 0.1 was assumed for the contact interface, consistent with typical values reported in the literature.
2.2.2 Material Properties
The gears were assumed to be made of a typical steel alloy with the following material properties:
- Elastic Modulus: 210 GPa
- Poisson’s Ratio: 0.3
- Density: 7800 kg/m³
- Yield Strength: 600 MPa
2.2.3 Boundary Conditions
For static analyses, the gears were constrained to prevent rigid body motion while applying a torque to the input shaft. For dynamic analyses, rotational velocities were applied to simulate operational conditions.
3. Static Simulation Results
3.1 Two-Axis Non-Parallelism
To investigate the effect of two-axis non-parallelism, the active gear axis was twisted outward by varying angles (0.2°, 0.4°, and 0.6°) while keeping the driven gear axis aligned. The resulting contact stresses under these conditions were analyzed.
Table 2. Contact Stress Variations with Two-Axis Non-Parallelism
| Twist Angle (°) | Contact Stress (MPa) – Active Gear | Contact Stress (MPa) – Driven Gear |
|---|---|---|
| 0.0 | 600 | 650 |
| 0.2 | 680 | 720 |
| 0.4 | 800 | 880 |
| 0.6 | 950 (Approaching Limit) | 1000 (Approaching Limit) |
The results indicate that as the twist angle increases, the contact stresses on both gears rise significantly. The maximum allowable twist angle, considering a safety margin, is determined to be ≤0.4°.
3.2 Tooth Side Clearance
Tooth side clearance was simulated by introducing lateral offsets (0.2 mm, 0.4 mm, and 0.6 mm) between the teeth of the mating gears. The contact stresses under these conditions were analyzed.
Table 3. Contact Stress Variations with Tooth Side Clearance
| Tooth Side Clearance (mm) | Contact Stress (MPa) – Active Gear | Contact Stress (MPa) – Driven Gear |
|---|---|---|
| 0.0 | 600 | 650 |
| 0.2 | 650 | 700 |
| 0.4 | 700 | 780 |
| 0.6 | 750 | 850 (Within Safe Limit) |
The analysis shows that while the contact stresses increase with tooth side clearance, they remain within the safe limit even at 0.6 mm clearance. However, dynamic analyses were further conducted to confirm the permissible limits.
4. Dynamic Simulation Results
4.1 Two-Axis Non-Parallelism (Dynamic)
Dynamic simulations were performed for twist angles of 0.2° and 0.4° to assess their impact on dynamic contact stresses.
Table 4. Dynamic Contact Stress Variations with Two-Axis Non-Parallelism
| Twist Angle (°) | Dynamic Contact Stress (MPa) – Active Gear | Dynamic Contact Stress (MPa) – Driven Gear |
|---|---|---|
| 0.2 | 700 (17% Increase) | 780 (20% Increase) |
| 0.4 | 850 (42% Increase) | 980 (49% Increase) |
The results demonstrate a more pronounced increase in dynamic contact stresses compared to static conditions. Consequently, the permissible twist angle is revised downwards to ≤0.2° to ensure operational safety.
4.2 Tooth Side Clearance (Dynamic)
Dynamic simulations were also performed for tooth side clearances of 0.2 mm, 0.4 mm, and 0.6 mm.
Table 5. Dynamic Contact Stress Variations with Tooth Side Clearance
| Tooth Side Clearance (mm) | Dynamic Contact Stress (MPa) – Active Gear | Dynamic Contact Stress (MPa) – Driven Gear |
|---|---|---|
| 0.2 | 720 (11% Increase) | 770 (10% Increase) |
| 0.4 | 780 (11% Increase) | 860 (10% Increase) |
| 0.6 | 880 (17% Increase) | 960 (Exceeding Safe Limit) |
The dynamic analyses reveal that while 0.2 mm and 0.4 mm clearances remain within safe limits, a clearance of 0.6 mm exceeds the allowable dynamic contact stress, necessitating a revision of the permissible limit to ≤0.4 mm.
5. Discussion
The comprehensive finite element simulations conducted in this study provide valuable insights into the effects of assembly errors on the mechanical behavior of helical gears in heavy truck transmissions.
5.1 Two-Axis Non-Parallelism
Static and dynamic analyses consistently show that two-axis non-parallelism significantly increases contact stresses on both active and driven gears. While static analysis suggests a maximum tolerable twist angle of 0.4°, dynamic analysis reveals a more conservative limit of 0.2° to ensure operational safety and reliability.
5.2 Tooth Side Clearance
Although static analyses indicate that tooth side clearances up to 0.6 mm remain within safe contact stress limits, dynamic analyses highlight the importance of considering dynamic effects. The resulting permissible limit of 0.4 mm ensures that even under dynamic loading conditions, the gears operate safely within their material limits.
6. Conclusion
This paper presents a systematic approach to determining permissible assembly errors in helical gears of heavy truck transmissions using finite element simulation. By analyzing both static and dynamic contact stresses under conditions of two-axis non-parallelism and tooth side clearance, the study provides quantitative limits for these errors.
The key findings are:
- The maximum allowable two-axis non-parallelism angle is ≤0.2° to ensure safe operation under dynamic loading.
- The maximum permissible tooth side clearance is ≤0.4 mm to maintain contact stresses within safe limits during both static and dynamic conditions.
These results offer practical guidelines for engineers involved in the assembly of heavy truck transmissions, ensuring optimal gear performance and extended service life. Future work could extend this research by investigating the combined effects of multiple assembly errors and by incorporating more realistic material behavior models.