Failure of gear core of electric rock drill

The gear core of the electric rock drill is composed of 11 parts. During its operation, it is required to apply 1800-2000 times / min of impact cycles, 200 times / min of torsion cycles and 70-100mpa of impact force to the drill rod. Except for the shell, all...