I have spent a considerable part of my engineering practice examining why sliding screw gears behave so differently depending on the lubrication regime in which they operate. Sliding screw gears are used primarily to transmit power while converting rotary motion into linear motion. The fundamental working principle is that two mutually contacting helical working flanks slide against each other, and the load is carried by the projected contact area of those flanks. In many ordinary applications, oil lubrication keeps the friction coefficient low and the wear rate acceptable. However, in certain specific situations, such as connections inside a gas circuit, oil lubrication is simply not permissible because the lubricant would contaminate the gas path. In those cases the screw gears must operate under dry friction. Under oil lubrication, a micro hydrodynamic pressure film forms between the screw flanks and provides effective separation and lubrication of the transmission surfaces. Under dry friction, however, the operating conditions and the available space often restrict any such film from forming, and the screw gears are prone to premature failure. My objective in this article is to explain, from a theoretical standpoint, why the wear resistance of sliding screw gears is insufficient in dry friction, and to describe measures that can be taken to improve it.
Sliding screw gears have the advantages of simple structure, convenient machining, and smooth operation, but they also exhibit large frictional resistance and rapid wear. The dominant failure mode of screw gears is wear of the nut thread. Under dry friction, the surface film on the metallic materials is easily worn away during service. Once the surface film is destroyed, the friction coefficient increases sharply. After prolonged operation, friction damage appears between the mating members, a certain amount of wear debris is generated on the contact surfaces, and this debris increases the probability of adhesive wear. I therefore treat the friction pair as a system in which surface topography, material hardness, contact pressure, and lubrication state all interact, and I analyze each of these factors in turn.

Surface Condition of the Mating Materials
A long series of theoretical studies and modern precision instrument measurements have shown that even with ultra precision machining, a real machined surface inevitably retains traces of the cutting tool. It is impossible for a machined surface to be absolutely flat and smooth. From a microscopic point of view, therefore, every machined surface is uneven. The same is true of the helical flanks of screw gears. The microscopic surface of a fresh flank consists of three components: the actual surface shape deviation, the waviness, and the surface roughness. When screw gears have run in for a period of time, the surface roughness is essentially worn away, and the microscopic surface then consists of only two components: the shape deviation and the waviness. This transition is important because it changes the nature of the contact from an asperity dominated contact into a broader, more conformal contact.
After running in, many tiny wedge shaped gaps exist between the helical flanks of the screw gears. Because these gaps are extremely small, they easily become filled with wear debris. A small amount of debris is actually beneficial, because it favors the formation of an oxide film and, to a certain extent, prevents direct metal to metal contact between the flanks. When the amount of debris becomes excessive, however, a series of side effects appears. Wear and heat generation both increase, and the debris itself becomes an abrasive third body that accelerates material removal from the screw gears. I have observed in practice that the transition from a beneficial debris population to a harmful one is not sharply defined, and it depends strongly on the load, the sliding speed, and the clearance between the flanks.
Material Hardness and Its Role in Screw Gear Pairs
According to the characteristics of engineering materials, if two materials have similar composition or similar hardness, and if a pressure exists between the contacting surfaces of the two parts while they move relative to each other without lubrication, then the two parts made of similar materials easily seize and adhere to one another. Two parts of similar hardness, on the other hand, easily scratch each other, which produces sluggish motion or even jamming. Screw gears are a loaded relative motion pair, so they require materials that are different from one another and that possess a certain hardness difference. In a steel on steel friction pair, the compositions of the two steels are similar and their hardnesses are also similar. Applying a metal oxide film or a coating can increase the hardness of one member relative to the other, which helps to establish a hardness difference and, at the same time, forms a dry film lubrication layer between the mating members. The establishment of a controlled hardness difference is, in my experience, one of the most reliable ways of preventing adhesive failure in screw gears.
Wear Resistance Check for Sliding Screw Gears
The wear resistance of sliding screw gears is checked by means of the working pressure ratio. The working pressure ratio is calculated from the axial load, the pitch diameter, the working height of the thread, and the number of thread starts. The governing expression is
$$p=\frac{F}{\pi d_2 h n}\le P_p$$
In this expression, F is the axial load in newtons, d2 is the pitch diameter of the screw in millimeters, h is the working height of the thread in millimeters, Pp is the allowable pressure ratio in newtons per square millimeter, and n is the number of thread starts. The quantity p is the mean contact pressure on the projected area of the helical flanks of the screw gears. Because the load is carried over the projected area, and because the projected area grows in proportion to the number of starts, the pressure ratio is inversely proportional to the number of starts. This simple relationship has a direct and useful consequence for the design of highly loaded screw gears.
At low speed and with good lubrication, the allowable pressure ratio for a steel on steel sliding screw gear pair is in the range of 7.5 to 13 N·mm−2. I was unable to find a published allowable pressure ratio for a steel on steel sliding screw gear pair operating in the dry friction regime. In order to investigate the relationship between the friction coefficient and the allowable pressure ratio, I collected the friction coefficients and allowable pressure ratios for steel on steel and steel on bronze pairs under conditions of good lubrication. The collected values are summarized in Table 1.
| Friction pair material | Friction coefficient | Allowable pressure ratio (N·mm−2) |
|---|---|---|
| Steel on steel | 0.11 to 0.17 | 7.5 to 13 |
| Steel on bronze | 0.06 to 0.08 | 18 to 25 |
For the friction coefficient entries in the table, the larger value applies at starting and the smaller value applies during running. When I analyzed the data in Table 1, I found that for a given friction pair material the friction coefficient and the allowable pressure ratio are approximately inversely proportional to one another. This observation can be expressed as a proportionality between the allowable pressure ratio and the reciprocal of the friction coefficient. I used this conclusion to derive the allowable pressure ratio for a steel on steel sliding screw gear pair operating in the dry friction regime.
Under dry friction, the friction coefficient of a clean steel on steel friction pair is 0.78, the friction coefficient of a steel on steel friction pair covered by an oxide film is 0.27, and the friction coefficient of a lubricated steel on steel friction pair is 0.11. On the basis of the inverse proportionality between the allowable pressure ratio and the friction coefficient, the allowable pressure ratio in the dry friction regime can be estimated from the allowable pressure ratio in the lubricated regime by the relation
$$P_{p,\text{oxide}}=\frac{\mu_{\text{lubricated}}}{\mu_{\text{oxide}}}\,P_{p,\text{lubricated}}$$
where the subscripts indicate the lubrication state to which each quantity refers. When the allowable pressure ratio of the lubricated pair is taken at its maximum value, the allowable pressure ratio of the steel on steel sliding screw gear pair in the dry friction regime with an oxide film present becomes
$$P_{p,\text{oxide}}=13\times\frac{0.11}{0.27}=5.3\ \text{N}\cdot\text{mm}^{-2}$$
When the allowable pressure ratio of the lubricated pair is taken at its minimum value, the corresponding result is
$$P_{p,\text{oxide}}=7.5\times\frac{0.11}{0.27}=3.0\ \text{N}\cdot\text{mm}^{-2}$$
The allowable pressure ratio in the dry friction regime is therefore substantially smaller than the allowable pressure ratio in the lubricated regime. This is one of the central reasons why screw gears that perform satisfactorily with oil lubrication can fail quickly when the oil is removed. In the dry friction regime, the oxide film is easily worn away during service. Once the surface film is destroyed, the friction coefficient changes from 0.27 to 0.78, which is a sharp increase. The increased friction coefficient lowers the effective allowable pressure ratio still further and drives the screw gears into a regime in which adhesive wear and seizure become very likely. This sequence of events leads to failure of the screw gear transmission and can cause damage to the surrounding equipment.
For completeness, I also estimated the allowable pressure ratio for a perfectly clean steel on steel screw gear pair in dry friction, using the clean surface friction coefficient of 0.78. The results are collected in Table 2 together with the oxide covered results.
| Lubrication state of the steel on steel screw gears | Friction coefficient μ | Allowable pressure ratio (N·mm−2) |
|---|---|---|
| Oil lubricated | 0.11 | 7.5 to 13 |
| Dry friction, oxide film present | 0.27 | 3.0 to 5.3 |
| Dry friction, clean metallic surface | 0.78 | 1.1 to 1.8 |
The clean surface values in the last row of Table 2 were obtained from the same inverse proportionality relation, using 0.11 divided by 0.78 as the scaling factor. They represent a limiting case that should be avoided in any practical screw gear design. It is worth noting that the allowable pressure ratio in the dry friction regime with an oxide film is roughly forty percent of the lubricated value, while the clean surface value is only about fourteen percent of the lubricated value. These ratios make it clear that the margin available in dry friction is small, and that any loss of the protective surface film consumes most of the remaining margin.
Friction Torque in Sliding Screw Gears
The friction torque of a sliding screw gear pair is calculated from the axial load, the pitch diameter, the lead angle, and the equivalent friction angle. The governing expression is
$$T_1=\frac{1}{2}d_2 F\tan(\gamma+\rho_v)$$
In this expression, F is the axial load in newtons, d2 is the pitch diameter of the screw in millimeters, γ is the lead angle of the helix, and ρv is the equivalent friction angle of the screw gear pair. According to this expression, for a given operating condition the friction torque depends only on the equivalent friction angle of the screw gears, because the axial load, the pitch diameter, and the lead angle are fixed by the design. The equivalent friction angle is itself related to the friction coefficient and the thread profile angle by
$$\rho_v=\arctan\frac{\mu}{\cos(\alpha/2)}$$
where μ is the friction coefficient and α is the thread profile angle. Combining the two expressions shows that when the friction coefficient μ increases, the equivalent friction angle ρv increases, and consequently the friction torque T1 of the screw gears increases. When an oxide film is present, the friction coefficient is relatively small, so the friction torque is moderate. After the oxide film fails, the friction coefficient increases significantly, and the friction torque T1 rises accordingly. The rise in friction torque reduces the mechanical efficiency of the screw gears and increases the heat generated at the flanks, which in turn accelerates film breakdown and wear. This positive feedback loop is the mechanism by which a screw gear pair can move from mild wear to severe adhesive damage in a relatively short time.
The sensitivity of the friction torque to the friction coefficient can be illustrated by evaluating the equivalent friction angle for several values of μ at a fixed thread profile angle. Taking a thread profile angle of sixty degrees, the half angle term cos(α/2) is equal to cos(30°), which is approximately 0.866. Table 3 lists the resulting equivalent friction angles and the corresponding tangent factors for the friction torque expression.
| Friction coefficient μ | Equivalent friction angle ρv (degrees) | tan(ρv) |
|---|---|---|
| 0.11 | 7.24 | 0.127 |
| 0.27 | 17.31 | 0.312 |
| 0.78 | 42.00 | 0.900 |
The values in Table 3 show that the tangent factor associated with the friction angle grows by a factor of about seven when the friction coefficient increases from the lubricated value to the clean surface value. This growth is only partly offset by the lead angle term in the total torque expression, so the net effect on the friction torque of the screw gears is large. I emphasize this point because it explains why a screw gear pair that feels smooth during assembly can become extremely difficult to operate after only a modest amount of dry running.
Factors That Influence the Friction Coefficient of Screw Gears
When the materials of the screw gears are steel on steel and the pair operates under dry friction, the steel on steel combination is prone to adhesion when the oxide film or the lubricating film fails, which causes failure of the screw gear transmission. The friction coefficient in a friction pair system is affected by many factors, including the matching properties of the material pair, the static contact time, the magnitude of the normal load, the loading rate, the rigidity and elasticity of the friction pair, the sliding velocity, the contact geometry and physical properties of the friction surfaces, and the chemical action of the surrounding medium. Because so many factors are involved, the friction coefficient of screw gears is not a fixed material constant, and it can vary considerably from one application to another. Applying lubrication to the friction pair reduces and stabilizes the friction coefficient, which is an effective way of improving the wear resistance of screw gears. Table 4 summarizes the principal factors and the direction in which they typically influence the friction behavior of screw gears.
| Influencing factor | Typical effect on friction of screw gears |
|---|---|
| Material pair matching | Similar composition and hardness promote adhesion |
| Static contact time | Longer contact increases junction growth and friction |
| Normal load magnitude | Higher load increases real contact area and friction |
| Loading rate | Rapid loading can raise the initial friction peak |
| Rigidity and elasticity | Compliant pairs redistribute load and alter friction |
| Sliding velocity | Velocity affects film formation and flash temperature |
| Surface geometry and properties | Roughness and waviness change contact pressure |
| Environmental medium | Oxygen and moisture promote or destroy oxide films |
Measures for Improving the Wear Resistance of Screw Gears
Sliding screw gears operating in the dry friction regime are used mainly in applications with special requirements. When the dimensions and the axial load cannot be adjusted, measures such as dry film lubrication, electroplated or chemically deposited layers, hard coatings, or a change in the number of thread starts can be adopted to improve the wear resistance of the screw gear pair. I discuss each of these measures in the following paragraphs and compare them in Table 5.
Dry Film Lubrication
Dry film lubricants can significantly reduce the friction coefficient of metallic materials and reduce the amount of wear, and they also possess a relatively high load carrying capacity. Dry film lubricants such as molybdenum disulfide have excellent pressure resistance and lubricating performance, and they can form a strongly adhering film on a metal surface. The surface roughness of a transmission thread flank is typically about 1.6 μm, while the thickness of a molybdenum disulfide lubricating film is usually on the order of a micrometer. Because the film thickness is of the same order as the roughness, many potential slip planes can exist within the film, and these slip planes can reduce friction fully and effectively. Applying a dry film lubricant therefore reduces the friction torque of screw gears. In my assessment, dry film lubrication is the least invasive of the available measures, because it does not require any change to the dimensions or the material of the screw gears, and it can be applied to existing hardware. Its main limitation is that the film has a finite life, and once the film is worn through the protection is lost.
Electroless Nickel Plating
The hardness of an electroless nickel deposit is generally in the range of 400 to 700 HV, and after appropriate heat treatment it can be increased further, so its wear resistance is good. The deposit bonds well to common substrates such as steel and copper. By adjusting the phosphorus content appropriately, the hardness, corrosion resistance, and wear resistance of the nickel layer can be improved. The deposit thickness is uniform and is typically about 0.01 mm. Before plating, the part should be machined to the pre plating dimension so that after plating the final dimension is achieved. The friction coefficient of electroless nickel is small, its non adhesive character is good, its wear resistance is high, and its surface possesses a degree of self lubrication. Tests have shown that electroless nickel plating can improve the wear resistance of screw gear pairs. I consider electroless nickel plating particularly suitable for the nut member of a screw gear pair, because the uniform thickness allows the thread geometry to be preserved within close tolerances.
Diamond Like Carbon Coating
Diamond like carbon, usually abbreviated as DLC, is a metastable amorphous carbon film composed of sp3 hybridized carbon, which has diamond like characteristics, and sp2 hybridized carbon, which has graphite like characteristics. It possesses performance characteristics similar to those of diamond, including high hardness, good chemical inertness, excellent wear resistance, and an extremely low friction coefficient, which makes it very suitable as an anti friction coating. By exploiting the wear resistance and lubricity of a DLC film, the wear resistance of transmission components can be effectively improved and the service life of the parts can be extended. Under extreme pressure conditions, the sp3 hybridized carbon transforms into sp2 hybridized carbon, which provides a self lubricating effect. After I applied a DLC coating to screw gears and carried out transmission tests, very fine black graphite like particles were found on the threads, and the friction torque was significantly reduced, which confirms that the DLC coating provides a self lubricating action. In addition, the hardness of the DLC film is higher than that of electroless nickel. If the nut is given an electroless nickel plating and the screw is given a DLC coating, the requirement of a hardness difference between the members of the screw gear pair is satisfied. This combination provides double protection of the screw gear pair and significantly improves wear resistance.
Double Start Threads
From the working pressure ratio expression given earlier, the working pressure ratio is inversely proportional to the number of thread starts. When the pitch diameter of the screw, the working height of the thread, and the axial load are held constant, the working pressure ratio of a double start thread is one half of the working pressure ratio of a single start thread. By adjusting the number of thread starts, the wear resistance of screw gears can therefore be improved and the service life of the transmission components can be extended. I regard the change of thread starts as a purely geometric measure, because it achieves the improvement without introducing any additional surface treatment or coating, and it is therefore attractive when the manufacturing process must remain simple. The trade off is that a multi start thread has a larger lead angle for a given lead, which changes the self locking behavior and the efficiency of the screw gears, so the change must be evaluated together with the actuation and braking requirements of the application.
| Measure | Mechanism | Typical hardness or thickness | Effect on screw gears |
|---|---|---|---|
| Dry film lubrication | Lamellar slip within the film | Micrometer order thickness | Lower friction torque, reduced wear |
| Electroless nickel plating | Hard, non adhesive deposit | 400 to 700 HV, about 0.01 mm | Improved wear resistance, self lubrication |
| Diamond like carbon coating | sp3 to sp2 transformation under pressure | Higher hardness than nickel | Very low friction, self lubrication |
| Double start thread | Increased projected contact area | Not applicable | Pressure ratio halved |
Combined Design Strategy for Dry Running Screw Gears
In my design practice I treat the wear resistance of dry running screw gears as a system problem rather than a materials problem alone. The first step is always to compute the working pressure ratio from the axial load, the pitch diameter, the working height, and the number of starts, and to compare the result with an allowable pressure ratio that is appropriate to the actual lubrication state. The allowable pressure ratio for dry friction is much lower than the value quoted for oil lubricated steel on steel screw gears, as the calculations in Table 2 demonstrate. If the computed pressure ratio exceeds the dry friction allowable value, then either the contact area must be increased, for example by using a double start thread, or the friction coefficient must be reduced and stabilized, for example by applying a dry film lubricant or a hard coating.
The second step is to ensure that a controlled hardness difference exists between the two members of the screw gear pair. Similar compositions and similar hardnesses promote adhesion, while a deliberate hardness difference suppresses it. A practical combination that I have found effective is a chemically deposited nickel layer on the nut and a diamond like carbon coating on the screw. This pairing satisfies the hardness difference requirement and simultaneously provides a low friction interface, because the DLC film supplies a self lubricating graphite like transfer layer under extreme pressure.
The third step is to verify the friction torque under the worst credible friction coefficient. The friction torque expression shows that the torque depends on the equivalent friction angle, which in turn depends on the friction coefficient and the thread profile angle. Because the friction coefficient can rise sharply when a protective film fails, the actuation system must be sized with enough margin to operate the screw gears even when the friction coefficient reaches the clean surface value. Table 3 shows that the tangent factor at a friction coefficient of 0.78 is about seven times the value at a friction coefficient of 0.11, so the torque margin requirement is substantial.
The fourth step is to consider the debris population within the wedge shaped gaps between the flanks. A small amount of debris is beneficial because it promotes oxide film formation and prevents direct metal contact. An excessive amount of debris is harmful because it increases wear and heat generation. Design features that allow fine debris to be flushed or retained in a controlled manner, together with surface treatments that resist adhesion, help to keep the debris population in the beneficial range. In my experience, the combination of a hard, non adhesive coating on one member and a softer, conformable coating on the other member produces a favorable debris regime, because the debris that forms is fine and relatively benign.
Analytical Summary
The analysis presented above can be summarized in a compact form. The wear resistance criterion for screw gears is the inequality between the working pressure ratio and the allowable pressure ratio. The allowable pressure ratio scales approximately with the reciprocal of the friction coefficient, so the dry friction allowable pressure ratio for steel on steel screw gears is only about three to five newtons per square millimeter when an oxide film is present, and only about one to two newtons per square millimeter when the surfaces are clean. The friction torque of the screw gears is governed by the equivalent friction angle, which increases sharply with the friction coefficient. The transition from an oxide covered surface to a clean metallic surface therefore produces a simultaneous reduction in the allowable pressure ratio and a simultaneous increase in the friction torque, which is precisely the combination that leads to adhesive failure and seizure. Table 6 restates the key numerical relationships.
| Quantity | Symbol | Expression or value |
|---|---|---|
| Working pressure ratio | p | p = F / (π d2 h n) |
| Allowable pressure ratio, lubricated steel on steel | Pp | 7.5 to 13 N·mm−2 |
| Allowable pressure ratio, dry with oxide film | Pp,oxide | 3.0 to 5.3 N·mm−2 |
| Allowable pressure ratio, dry clean surface | Pp,clean | 1.1 to 1.8 N·mm−2 |
| Friction torque | T1 | T1 = 0.5 d2 F tan(γ + ρv) |
| Equivalent friction angle | ρv | ρv = arctan[ μ / cos(α/2) ] |
Practical Recommendations
On the basis of the analysis and the numerical evaluations, I recommend the following practical approach for sliding screw gears that must operate in dry friction. First, compute the working pressure ratio and compare it with the dry friction allowable value rather than the lubricated value. Second, select a friction pair that provides a deliberate hardness difference, and consider a nut with electroless nickel plating mated to a screw with a diamond like carbon coating. Third, apply a dry film lubricant such as molybdenum disulfide where the film life is sufficient for the required service interval, and verify the film thickness relative to the surface roughness of the screw gear flanks. Fourth, where the pressure ratio is excessive and the geometry can be changed, convert a single start thread into a double start thread so that the working pressure ratio is halved. Fifth, verify the friction torque at the worst credible friction coefficient and provide adequate actuation margin, because the friction torque of the screw gears rises steeply as the friction coefficient increases. Finally, monitor the debris condition during testing, because a fine, well dispersed debris population indicates that the surface films are functioning, while a coarse, agglomerated debris population indicates that adhesive wear has begun.
Concluding Remarks
Sliding screw gears perform acceptably when oil lubrication is available, because the lubricant maintains a low and stable friction coefficient and forms a micro hydrodynamic film between the flanks. In certain applications where oil lubrication cannot be used, screw gears operate in the dry friction regime and often suffer severe adhesion. My analysis of the surface condition and the material hardness of the friction pair, together with the wear resistance check and the friction torque calculation, provides a theoretical explanation of why the wear resistance in dry friction is insufficient. The change in the friction coefficient between different states is the principal cause of the deficiency, because the allowable pressure ratio is inversely related to the friction coefficient while the friction torque increases with it. To meet the wear resistance and lubrication requirements of screw gears, I have described measures based on dry film lubrication and surface strengthening. Dry film lubrication, electroless nickel plating, diamond like carbon coating, and double start threads can all improve the wear resistance of sliding screw gears. When these measures are selected rationally in accordance with the actual operating conditions, the ability of the material to resist adhesion and seizure is improved, and the service life of the screw gears is extended.