Influence of part shape on deformation of truck gear
The shape of parts is a very important factor affecting the deformation size and deformation trend of heat treatment, which […]
The shape of parts is a very important factor affecting the deformation size and deformation trend of heat treatment, which […]
Compared with similar products in advanced countries, the quality of truck gears in China lags far behind, with an average […]
Carburizing and quenching of truck gears is a key process in the process of gear quality control. Many key characteristics […]
The research on heat treatment deformation control of heavy truck gearbox gear is of great practical significance and great practical […]
At present, foreign automobile manufacturers generally adopt isothermal annealing treatment for truck gear forging blank, and specify different isothermal annealing […]
As we all know, the quality of gears is influenced not only by the steel itself, but also by the […]
Foreign tests have proved that the supercooled austenite decomposition products during surface quenching of carburized steel are the main reason […]
China’s truck gear steel basically follows the brand of the former Soviet Union. For a long time in the past, […]
1. Test purpose Our company adopts high-grade and high-quality zocrmntih steel with 6 bandwidths according to the steel factory standard. […]
1. Introduction to truck gear processing The cold working routes of the three parts are basically the same: forging – […]
The metallurgical quality of steel for truck gear has the following requirements: 1.End hardenability At present, the bandwidth control of […]
Taking 9t one speed gear parts as an example, the effects of different pre heat treatment methods on the deformation […]
Three typical parts of heavy truck gearbox hc7s-120: first and second speed gear sleeve (representative of thin-walled castings), fourth speed […]
Material quality is affected by multiple factors. Different origin, smelting methods, quality categories and supply forms of truck bevel gear […]
From the above analysis of the service conditions and failure forms of gears, it is proposed that the performance requirements […]
1. Effect of pre heat treatment on cylindrical gear deformation Before 2010, our company adopted the ordinary normalizing method for […]
The gearbox gear of heavy truck is one of the three major products of ZHY Gear. It has been supporting […]
The influence of material quality on the quality of truck helical gear has attracted more and more attention. The unstable […]
The deformation of heavy truck gearbox gear after carburizing and quenching is caused by the gear in the process of […]
With the continuous development of China’s automobile industry and national economy year-on-year, the heavy vehicle industry has also entered a […]
At the beginning of this century, the German automobile industry used high Ni alloy steel to produce high load truck […]
Heavy truck gear refers to all kinds of gears in the gearbox of heavy truck. The automobile gearbox is located […]