Trial production results of spur gear (sun gear)
The combined die is the key component for continuously extruding the external teeth of spur gear. The combined die adopts […]
The combined die is the key component for continuously extruding the external teeth of spur gear. The combined die adopts […]
With the development of mechanics and computer simulation technology, the research on fatigue crack of spur gear has made great […]
Bevel gear is widely used in mechanical transmission, especially in automobile transmission mechanism. The traditional bevel gear processing adopts the […]
When the module, number of teeth, helix angle and process parameters of helical gear are consistent, three groups of different […]
As a typical transmission part, bevel gear is widely used in many industries, such as aviation, aerospace, automobile, instrument and […]
① Hot forging blank The material of spur gear in truck wheel reducer is 20CrMnTi. Solid bar is selected as […]
According to the statistics of scholars, most of the mechanical component failures belong to fatigue failure, accounting for 50% – […]
In the process of helicall gear design, CAD / CAM / CAE integrated software UG is adopted. Combining the three-dimensional […]
The difference between helical gear and spur gear is that the teeth of helical gear are distributed along the helix. […]
The cold extrusion precision plastic forming technology of spur gear has the advantages of saving materials, improving production efficiency, ensuring […]
The continuous extrusion forming process of the external teeth of the spur gear is the same as that described above. […]
(1) The parametric modeling of helical gear is carried out by using three-dimensional modeling software UG. After parametric modeling, helical […]
Through the numerical simulation analysis of the closed die forging of helical gear, the parameters such as temperature, friction factor, […]
Due to the formula of indexing circle diameter d = mz, it can be seen that the diameter of the […]
The three forming process schemes will be comprehensively evaluated and analyzed from the three aspects of material utilization, production efficiency […]
1.Influence of blank temperature The blank temperature of spiral gear is 20 ° C, 450 ° C and 850 ° […]
Closed die forging process is a traditional one-step process. Its forming process is simple and convenient for analysis and research. […]
For a long time, for helical gear designers, the design or development of a process scheme is basically based on […]
In order to clearly see the deformation process of inner and outer teeth in the forming process of spur gear […]
All teeth on helical cylindrical gears are the same and have unified characteristics. The normal tooth profile will be generated […]
In recent ten years, with the rapid development of computer hardware and software technology and the in-depth study of material […]
Taking the forging compound forming process of driving and driven spiral bevel gears as the research object, the feasibility of […]
The main feature of die forging is that the diameter of outer circle and inner hole of automobile rear axle […]
The precision plastic forming part of spiral gear has high dimensional accuracy and less machining allowance. It only needs a […]
At present, the research on precision plastic forming of bevel gear and spur gear has made great progress and has […]
Taking a certain type of automobile rear axle spiral bevel gear as the research object, taking the product part drawing […]
Y. Qin and R. Balendra used abaques simulation software to study the elastic deformation of the die cavity in the […]
The precision forming technology of cylindrical gear comes from Germany. As early as the 1950s, due to the lack of […]
Precision near net shape forming of spiral gear belongs to less and no cutting technology. Due to its outstanding advantages […]
The numerical simulation analysis is based on the assumption of rigid plastic finite element model. Properly combine and simplify the […]
Taking the sun gear in a truck wheel reducer as the research object, its part drawing and three-dimensional solid model […]
Spiral gears include spiral cylindrical gear and spiral bevel gear. As one of the most basic parts to transmit motion […]
1.Open die hot die forging Open die hot die forging is the earliest forging process of driven bevel gear. With […]
Warm forging of helical gear is a kind of plastic forming process with less and no cutting developed on the […]
1.Existing process of hot die forging (cross forging) Hot die forging of driving spiral bevel gear blank is the earliest […]
Because the composite casting and forging process used to produce automobile rear axle spiral bevel gear has not been applied […]
As the starting point of casting forging compound forming process, whether the process design of casting process and the control […]
The rolling forming process of spur gear improves the production efficiency and material utilization, shortens the processing process, and the […]
Research overview of spiral bevel gear forging at home and abroad and the application of numerical simulation technology in spiral […]
Based on the existing forming methods of driving and driven bevel gear blank of automobile rear axle, a new composite […]
The driving and driven spiral bevel gears of the automobile rear axle are the key parts of the automobile rear […]
At present, the better process methods for producing the driven helical gear blank of automobile rear axle at home and […]
Automobile rear axle gear is an important part of automobile drive system. Due to its poor working condition and heavy […]
The figure shows the metal velocity distribution of different strokes in the cold finishing process of spiral bevel gear, in […]
As the starting point of casting forging compound forming process, whether the process design of casting process and the control […]
1. Tooth surface contact analysis of spiral bevel gear Based on the above theoretical methods, the whole process design software […]
The cold / hot forging drawing is determined by the helical gear part drawing. The influence of the tooth shape […]
1.Load stroke curve Figure 1 shows the load stroke curve of hot die forging process of different taper schemes of […]
Shu Qifu once put forward the concept of “equivalent blank” to study the influence of taper on the forming process […]
Cold extrusion process is a production technology with high precision, high efficiency, high quality and low consumption, which is widely […]
1.Load stroke curve Fig. 1 is the load stroke curve of spiral bevel gear blank obtained according to the approximate […]
The figure shows the distribution of equal effect variation in the final step. From the figure, it can be seen […]
Referring to the tooth size of cold precision forging preform, the closed hot die forging die chamber is designed and […]
Fully referring to the idea of shunting method, it is decided to adopt the approximate trapezoidal tooth profile scheme with […]
Based on the design of process flow, the main purpose of closed hot die forging step is to realize the […]
The traditional tooth surface contact mainly includes transmission error and tooth surface contact area. At present, a new analysis method, […]
The basic forming process of spur gear has its own obvious advantages and disadvantages. It can only solve the problems […]
1.Load stroke curve Figure 1 shows the load stroke curve of preforms with different cold precision forging quantities according to […]
CATIA software is used to complete the three-dimensional modeling of upper die, lower die and cold precision forging preforms with […]
The forming quality of forgings directly determines the quality and service life of products. The surface finish of the straight […]