Research progress of automotive gear steel
Automobile gear is an important transmission part, which plays the role of transmitting power and changing speed and direction. Due […]
Automobile gear is an important transmission part, which plays the role of transmitting power and changing speed and direction. Due […]
In the process of automobile manufacturing, as an important part of the transmission system, the quality of the gear directly […]
Since the mid-1980s, China’s gear industry has developed rapidly. Due to the high requirements of technical parameters, the gear required […]
In the early automobile gear production, heat treatment induction quenching was widely used because of its high production efficiency, small […]
Heat treatment carbonitriding process is frequently used because it can effectively improve the depth of carburizing layer, obtain high hardness, […]
Heat treatment carburizing process can make gears have good comprehensive mechanical properties, so it is most widely used in the […]
Automobile gears are usually made of low-carbon alloy carburized steel. Gear blanks generally need to go through multiple cold and […]
The research object is a light truck drive axle, which is mainly composed of main reducer, axle housing, axle shaft, […]
Due to the complex contact problem of helical gear, further research is needed in the following aspects: ① Fully parametric […]
Based on the research of bionics theory, combined with the characteristics of automobile gear meshing transmission, and based on the […]
When the contact stress of automobile gear is too large, the plastic flow of tooth surface metal due to yield […]
In the high-speed and heavy-duty gear transmission of automobile gears, the pressure in the meshing area of the tooth surface […]
Fatigue pitting of the tooth surface of automobile gear is a common failure form of closed soft tooth surface gear […]
Traditionally, the methods to improve the wear resistance of gears are mainly to change the gear manufacturing materials or the […]
In automobile gear transmission, there are many different forms of tooth surface wear with different working conditions. There are mainly […]
In China’s automobile industry, the materials used for gears in the gearbox have mainly used the gear steel series of […]
In foreign countries, the carburized gear steel initially used is basically manganese steel and manganese chromium steel. For example, the […]
Through the friction and wear test, the comparative experimental research between the smooth sample and nine different pit bionic ring […]
According to different working conditions, gear transmission can be divided into closed type and open type; According to different use […]
Automobile gear transmission product development test refers to a series of tests required to check the design level and process […]
The main purpose of the durability test of automobile gear transmission system is to simulate the load conditions that the […]
Gear transmission product development test refers to a series of tests required to check the design level and process rationality […]
After studying and analyzing the research results on the forming of spiral bevel gear at home and abroad, it is […]
Based on the analysis of the forging process of the double spiral bevel gear of an automobile, the forming process […]
The driven spiral bevel gear of an automobile rear axle is taken as the research object, and its part structure […]
Figure 1 is the structure diagram of the designed precision forging part. Because the tooth surface of the spiral bevel […]
In the helical gear transmission of hybrid electric vehicle, although the rolling motion conditions are considered in the tooth surface […]
The meshing error of gear teeth mainly comes from the error caused by gear processing and installation. Machining error mainly […]
The planetary gear transmission system of hybrid electric vehicle studied is composed of composite planetary gear mechanism and parallel axis […]
In the cylindrical gear transmission system of hybrid electric vehicle, due to the need of lubrication and the manufacturing accuracy […]
Using the lumped parameter method, fully consider the nonlinear factors in the gear transmission system, such as time-varying meshing stiffness, […]
Barrel grinding can improve the tooth surface roughness and the fatigue life of automotive helical gears under certain conditions, and […]
In recent years, companies in Japan and Taiwan have studied and applied the spraying technology of composite materials containing MoS2 […]
Molybdenum disulfide (MoS2), as a high-quality solid lubricating material, has good antifriction, wear resistance and bearing capacity. Molybdenum disulfide (MoS2) […]
The application of manganese phosphate conversion coating process in improving the surface strength of transmission parts first appeared in the […]
As shown in the figure, the failure zone diagram of automobile gear transmission made by Nieman, Professor of Munich University […]
With the development of science and technology, as an important technology to introduce residual compressive stress, change the microstructure of […]
Strong shot peening can greatly increase the residual compressive stress near the surface of automobile gear, promote the transformation of […]
The automobile rack and pinion steering gear assembly is an important steering component of many automobiles. The automobile rack and […]
In the research of surface strengthening technology for bending fatigue strength of automobile gears, Japan has studied and developed various […]
The design of the main interface of the rack and pinion steering gear is very important in the process of […]
Perfect product criteria and reliable product design knowledge are the guarantee for the rapid establishment and correct design of product […]
Japan and Germany have done a lot of research in the basic research field of automobile gears. Steel roller test […]
Complete the parametric design analysis and research of automobile rack and pinion steering gear based on CATIA. In the implementation […]
The virtual assembly process is that the user changes the manual assembly operation process of the specified automobile rack and […]
Automobile rear axle is also called drive axle. It not only bears the load, but also acts as differential and […]
With the enhancement of China’s national strength, China’s scientific level has been greatly improved. At the same time, it has […]
The rack is an involute gear whose base circle radius is infinite, and its contour has changed from involute to […]
On the basis of studying a large number of relevant data at home and abroad, this paper makes an in-depth […]
The heat treatment strengthening technology of automobile gears should pay attention to the control of surface integrity, that is, to […]
Interference analysis is one of the important contents of virtual assembly design of automobile rack and pinion steering gear. After […]
The basic parameters of automobile steering gear mainly include the number of teeth, modulus, pressure angle, tooth width, displacement coefficient […]
General products are composed of one or many parts. In order to realize the parametric design of products, we must […]
This paper introduces automobile steering system and automobile rack and pinion steering gear, then introduces the current situation of automobile […]
After the above experimental analysis and referring to the metallographic inspection of Automobile Carburized Gears, it can be observed that […]
1. Analysis of fracture morphology of aluminum alloy automobile gear In order to analyze the fracture failure cause of aluminum […]
Gear is an important part of automobile transmission device, which has the functions of changing movement direction, changing speed and […]
Through gene analysis and basic performance experiment of automobile gear materials, it is very important to master the basic parameters […]
The automotive helical gear transmission system under various complex working conditions makes the surface strengthening technology of automotive helical gear […]
The fatigue damage of automobile gear tooth surface is caused by the repeated action of automobile gear on the tensile […]