Design of concave die for spiral bevel gear centripetal bearing structure
Figure 1 shows the engineering drawing of spiral bevel gear bearing structure female die. The outer diameter of the die […]
Figure 1 shows the engineering drawing of spiral bevel gear bearing structure female die. The outer diameter of the die […]
Swing rolling of spiral bevel gear is a processing method in which the blank is continuously and locally loaded by […]
In the swing rolling of spiral bevel gear, there are many factors affecting the forming quality and size of bevel […]
When using rigid viscoplastic finite element method to analyze metal plastic forming, the material meets the following assumptions: (1) ignoring […]
In recent years, some scholars have done a lot of research on the rotary forging process. The rotary forging of […]
Figure 1 shows the equivalent stress distribution diagram of closed die forging of spiral bevel gear. Under four reduction quantities, […]
1.Establishment of finite element model The finite element model is shown in Figure 1. The forging with gears is formed […]
Spiral bevel gear is one of the core parts of automobile engine to transmit power. It can transmit large load […]
When the module, number of teeth, helix angle and process parameters of helical gear are consistent, three groups of different […]
Taking the forging compound forming process of driving and driven spiral bevel gears as the research object, the feasibility of […]
Taking a certain type of automobile rear axle spiral bevel gear as the research object, taking the product part drawing […]
Y. Qin and R. Balendra used abaques simulation software to study the elastic deformation of the die cavity in the […]
1.Existing process of hot die forging (cross forging) Hot die forging of driving spiral bevel gear blank is the earliest […]
Because the composite casting and forging process used to produce automobile rear axle spiral bevel gear has not been applied […]
As the starting point of casting forging compound forming process, whether the process design of casting process and the control […]
Research overview of spiral bevel gear forging at home and abroad and the application of numerical simulation technology in spiral […]
The driving and driven spiral bevel gears of the automobile rear axle are the key parts of the automobile rear […]
Automobile rear axle gear is an important part of automobile drive system. Due to its poor working condition and heavy […]
The figure shows the metal velocity distribution of different strokes in the cold finishing process of spiral bevel gear, in […]
As the starting point of casting forging compound forming process, whether the process design of casting process and the control […]
1. Tooth surface contact analysis of spiral bevel gear Based on the above theoretical methods, the whole process design software […]
1.Load stroke curve Figure 1 shows the load stroke curve of hot die forging process of different taper schemes of […]
1.Load stroke curve Fig. 1 is the load stroke curve of spiral bevel gear blank obtained according to the approximate […]
The figure shows the distribution of equal effect variation in the final step. From the figure, it can be seen […]
Referring to the tooth size of cold precision forging preform, the closed hot die forging die chamber is designed and […]
The traditional tooth surface contact mainly includes transmission error and tooth surface contact area. At present, a new analysis method, […]
CATIA software is used to complete the three-dimensional modeling of upper die, lower die and cold precision forging preforms with […]
The optimal parameter scheme is numerically simulated and the forming process is analyzed. The following conclusions are obtained: (1) The […]
The figure shows the equivalent stress distribution diagram of spiral bevel gear at different strokes in the cold finishing process, […]
The risk of casting forging compound forming process is controllable and the process predictability is strong; Taking the product part […]
1. Part drawing analysis Figure 1 is the part drawing of the driven spiral bevel gear of the rear axle […]
Using traditional manufacturing technology to produce high-performance complex parts has become the bottleneck restricting the improvement of product quality and […]
The data obtained from the on-site measurement of the profile error of spiral bevel gear teeth are the readings XRK […]
Automobile rear axle (also known as drive axle) refers to the rear drive shaft and related components used to transfer […]
As one of the main transmission parts of automobile, the driven spiral bevel gear of automobile rear axle has great […]
Physical simulation is a method based on similarity theory and combined with experiment to study the essence and law of […]
Use CATIA three-dimensional mathematical modeling software to establish the three-dimensional mathematical models of the upper die and lower die in […]
In the process of metal plastic forming, most of the deformation work of metal plastic deformation will be transformed into […]
The analysis of metal flow law can make us more clearly understand the flow law of metal in the forming […]
Based on the generating principle, the profile error of gear teeth is measured on the machine, and the workpiece needs […]
Equivalent strain refers to the strain equivalent to unidirectional strain formed by the appropriate combination of various strain components in […]
During the precision forging process of the driven spiral bevel gear of the automobile rear axle, the load will change […]
Stress is the internal force per unit area, which reflects the stress of spiral bevel gear blank. Figures (a), (b), […]
It can be seen from the research that the change of finishing forming force is not only affected by the […]
Using CATIA V5R21 three-dimensional mathematical modeling software, the three-dimensional mathematical models of upper and lower dies and blanks in the […]
In the forming process of driven spiral bevel gear of automobile rear axle, the practical application process of precision forging […]
The blank size, forming temperature, forming speed, friction factor and die structure of the precision forging process of the driven […]
The node velocity reflects the speed of metal flow at the node at a certain movement time. Figures (a), (b), […]
Strain is a physical quantity indicating the size of deformation, the accumulation process of plastic deformation and the development process […]
The unreasonable selection of the finishing quantity will directly affect the filling condition of the tooth profile and the roughness […]
The speed of forming speed has a very important impact on the processing efficiency and quality of forgings. With the […]
For the process of precision forging the driven spiral bevel gear of automobile rear axle at different temperatures, the distribution […]
When the forming temperature distribution of the driven gear is different, the forming temperature distribution of the driven gear always […]
Analyze the stroke load curve of the forming process of the driven spiral bevel gear of the automobile rear axle […]
On ABAQUS software, the meshing process of spiral bevel gear is divided into 200 incremental steps. In the dynamic analysis, […]
The plasticity of metal is related to temperature. The higher the temperature, the better the plasticity of metal. For forging, […]
As shown in the figure, the equivariant distribution diagram of five spiral bevel gear blank size schemes is shown, in […]
As shown in the figure, the equivalent stress distribution diagram of five spiral bevel gear blank size schemes is shown, […]
The figure shows the travel load curves of five blank size schemes, in which (a) (b) (c) (d) (E) correspond […]
On the premise of the compound forming process of spiral bevel gear hot forging and cold finishing, combined with the […]