Research status of gear friction excitation in China and abroad
For the research of tooth surface friction, more attention is paid to the heating and energy consumption caused by friction, […]
For the research of tooth surface friction, more attention is paid to the heating and energy consumption caused by friction, […]
Three typical parts of heavy truck gearbox hc7s-120: first and second speed gear sleeve (representative of thin-walled castings), fourth speed
Material quality is affected by multiple factors. Different origin, smelting methods, quality categories and supply forms of truck bevel gear
The process tests of 9T 34556 speed gear sleeve with different heat treatment methods, different heat treatment process parameters and
In 1674, Danish astronomer Romer used the enveloping cycloid as the gear tooth profile to obtain the gear with conjugate
Through the process test of two different pre heat treatments on the deformation law of the parts after final carburizing
From the above analysis of the service conditions and failure forms of gears, it is proposed that the performance requirements
1. Test purpose Verifying the rationality of bevel gear process is an effective guarantee to reduce the heat treatment deformation
1. Test purpose Verify the influence of different pre heat treatment methods on the deformation of final carburized helical cylindrical
1. Effect of pre heat treatment on cylindrical gear deformation Before 2010, our company adopted the ordinary normalizing method for
Among the main factors affecting the gear heat treatment deformation, the only thing that can be improved by the heat
The automotive helical gear transmission system under various complex working conditions makes the surface strengthening technology of automotive helical gear
The gearbox gear of heavy truck is one of the three major products of ZHY Gear. It has been supporting
The influence of material quality on the quality of truck helical gear has attracted more and more attention. The unstable
The machining method and residual stress of spiral gear will have a certain influence on the deformation of carburized spiral
Forging can make the forging billet segregation, uniform structure and reduce the banded structure, which is conducive to reducing the
Figure 1 shows the equivalent stress distribution of spur gear under different cold shaping methods. During full tooth shaping, the
The deformation of heavy truck gearbox gear after carburizing and quenching is caused by the gear in the process of
The fatigue damage of automobile gear tooth surface is caused by the repeated action of automobile gear on the tensile
Through the speed field of precision forging of spiral bevel gear, the flow of metal blank in the forming process
The purpose of gear modification is to make the pressure distribution on the tooth surface as uniform as possible after
As shown in the table, the forging deformation force of open die forging and non flash die forging of spiral
With the continuous development of China’s automobile industry and national economy year-on-year, the heavy vehicle industry has also entered a
Due to these irreplaceable advantages, spiral bevel gear has been widely used as an important part in the transmission system
The dual frequency induction quenching process of bevel gear includes electromagnetic induction heating process and quenching cooling process. The temperature
The cutting parameters of gear hob include cutting depth, cutting speed and axial feed. The determination of these parameters should
At the beginning of this century, the German automobile industry used high Ni alloy steel to produce high load truck
Heavy truck gear refers to all kinds of gears in the gearbox of heavy truck. The automobile gearbox is located
① Aiming at the problems of serious tooth tip collapse, low material utilization, low forming accuracy and low die service
In the field of scientific research and engineering technology, numerical simulation is a basic research method that pays equal attention
Shot peening is a widely used method to improve the fatigue strength of automobile gears by mechanical means to produce
The automobile gear is in the state of continuous load operation. There are both rolling and sliding between the meshing
Automotive automatic transmission lubricating oil (ATF) not only meets the lubrication of automotive helical gears and bearings, but also undertakes
With the continuous improvement of automotive gear requirements and the continuous development of automotive gear surface processing engineering technology, the
The best effect of shot peening strengthening treatment of automobile gears is affected by the interaction of different conditions. The
The strength of automobile gear is mainly the bending fatigue strength and tooth surface contact fatigue strength of gear. Figure
Modulus is an important parameter of gear. When selecting automobile gear modulus, factors such as strength, noise, lightweight and processing
Gear is an important part for transmitting power in mechanical devices. The Japanese mechanical society has conducted systematic investigation and
In previous studies, the ideal model without error is used in the numerical simulation of cold shaping of spur gear.
(1) Mold and blank materials can be directly selected from the material library of DEFORM software. The mold material is
The mesh generation program of DEFORM-3D can divide the geometry into tetrahedral elements, and its mesh generation methods can be
The forging deformation force P of spiral bevel gear is determined by empirical formula: Where: C – shape complexity coefficient
Spiral bevel gear is the general name of bevel gear whose tooth surface pitch line (the intersection line of tooth
In order to facilitate calculation, the involute tooth profile of spiral bevel gear is simplified into linear tooth profile according
Combined with the actual needs of gear hobbing tools in automobile gear production line, select the problems often encountered in
Taking the spur cylindrical gear for truck wheel reducer as the research object, a new compound forming process scheme of
Based on the open die forging of spiral bevel gear, a new type of precision forging die without flash is
Custom gear manufacturing plays a crucial role in meeting the unique requirements of specialized applications across various industries. Unlike standard
Sizing belt is one of the key process parameters to ensure the forming of spur gears. Whether the length of
The numerical simulation of precision forging is to track and describe the forming process of the blank metal of the
The figure shows the new precision forging die structure of spiral bevel gear. The working part of the die is
By analyzing the forming characteristics of open die forging and the shape of spiral bevel gear forging, the plastic deformation
The figure is the area differential diagram of the large end of the tooth profile of spiral bevel gear. Let
As can be seen from Figure 1, the shape of spiral bevel gear is relatively complex, especially its tooth shape
1. Design principle of gear induction coil The size of the gear module plays an almost decisive role in the
ANSYS software itself has powerful meshing function, so ANSYS software is used for meshing. Import the 3D model built in
Determining the forging deformation force is a very important part of the metal plastic forming theory. The research on the
Some parts need teeth as a benchmark. For example, the time difference is generated by controlling the angle of the
The same parameters as the grinding test are used for simulation, and the simulation results are shown in Figure 1.
In order to ensure the smooth implementation of cold extrusion production and processing, in addition to having a pair of