Analysis of surface crack of s40c steel gear
According to the above inspection results, the cracking of steel gear tooth surface is caused by contact fatigue caused by […]
According to the above inspection results, the cracking of steel gear tooth surface is caused by contact fatigue caused by […]
In recent years, the research and application of CAD / CAPP Technology in gear mostly focus on the design of […]
The gear material of the failed rolling mill is 17CrNiMo6 steel, the modulus Mn is 9mm, the carburizing and quenching […]
Produced by a company φ 2100mm large forged gear blank with a weight of 6000kg was found to be cracked […]
Bevel gear is widely used in mechanical transmission, especially in automobile transmission mechanism. The traditional bevel gear processing adopts the […]
Velocity field is a vector to measure the flow of material in the process of plastic deformation. Through the observation […]
The rolling mill gear shaft with grinding cracks is made of 17CrNiMo6 steel, the modulus Mn is 18mm, the carburizing […]
Gear is an important basic part of mechanical products. Gear grinding is a finishing process of gear processing. Gear grinding […]
Swing rolling, namely swing rolling, also known as axial rolling, is a new plastic processing technology gradually and widely used […]
1. Processing with Norton 3SG60 grinding wheel (1) rough grinding: the 1st ~ 3rd cutters are in the form of […]
Figure 1 shows the driven bevel gear of rear axle in 46910 / 37 commercial vehicle. It can be seen […]
The general plastic precision forming process is precision die forging, which is a less cutting process gradually developed from general […]
The precision forging process of spiral bevel gear generally has some problems, such as difficult forming, difficult cavity filling, low […]
Taking the transmission gear of heavy equipment as the research object, the fatigue crack propagation and fatigue fracture of gear […]
In the process of EDM, the electrode will have a certain amount of burning loss, which will change the electrode […]
For the finish machining of hardened cylindrical gears, gear grinding technology is a common choice at present. On the premise […]
The model used for the numerical simulation of gear bending fatigue is the same as that used in the bending […]
Hypoid gear is widely used in aviation, automobile and other fields. As an important index to predict its dynamic performance, […]
When rolling the thick cylinder of the pier, the relationship between the feed rate s per revolution and the average […]
1. Technical analysis of forging process In offshore engineering, the requirements for large herringbone gears are relatively high. The original […]
When testing the bending fatigue of 42CrMo heavy equipment transmission gear by experimental method, the data results have obvious advantages, […]
The feed rate per revolution of the cone die is the reduction amount per revolution, which is the reduction amount […]
Before the formal bending fatigue test, the load level of the test needs to be determined. Pick two from the […]
For the five kinds of swing head motion trajectories in the figure, they are analyzed one by one as follows: […]
The bending fatigue characteristic curve and bending fatigue limit stress of the test gear shall be combined according to different […]
1. Advantages of large herringbone gear in aviation and ocean engineering The diameter of large gears used in aviation and […]
The motion track of the swing head refers to the projection track of any point on the axis of the […]
Figure 1 shows the front view of the temperature field on the single tooth profile surface and the middle section […]
Due to the eccentric load on the workpiece during rotary forging, the metal flow is uneven. If the preform is […]
The transmission gear of heavy equipment used in the bending fatigue test is designed based on the gear applied in […]
Among the key areas of China’s planning, marine engineering is the most important project and development field. Marine engineering includes […]
The so-called “thick piece” revolving body means that the thickness h is greater than or equal to the radius R […]
The test adopts the form of single tooth loading. It is necessary to design special fixtures according to the standard […]
The stress ratio r = 0.6, the number of cycles n corresponding to the stress intensity factor at the crack […]
The essence of swing rolling is a special two roll rolling. In the process of rotary forging, although the swing […]
In order to verify the correctness of the above crack propagation, the crack length and crack tip stress intensity factor […]
The cold rotary forging precision forming process of bevel gear is an advanced manufacturing technology. Its process design in actual […]
The equivalent stress at the crack tip under different crack inclination angles is extracted and plotted, and the equivalent stress […]
Hypothetical generating wheel is usually used to explain the machining process of bevel gear. It is a virtual bevel gear […]
The dynamic continuous growth of fatigue crack is realized by resetting the crack length each time. In the numerical simulation […]
Study the crack propagation law when the initial crack position H0 is 60mm, 62mm, 64mm, 66mm, 68mm and 70mm respectively, […]
Fig. 1 shows 150, 300, 500 and 1000 times SEM images of fatigue fracture in the instantaneous fracture zone. The […]
In the actual process of gear meshing, the maximum contact stress usually acts on the tooth surface of the pinion. […]
Under the continuous loading of cyclic loading and unloading, the slip band around the crack tip deforms, resulting in the […]
Hypoid gear is a bevel gear with central axis offset. The tooth surface surface of this type of gear is […]
At 3 000 n · The equivalent time-varying meshing parameters of hypoid gear in one cycle are calculated according to […]
The transmission error curves obtained by finite element method and classical TCA method are compared to verify the correctness of […]
In order to simulate the singularity and discontinuity of element displacement stress, it is realized by constructing the extended functions […]
According to the established contact fatigue finite element simulation model of hypoid gear transmission system, the finite element simulation software […]
It can be seen that the fracture clearly presents three regions with different morphological characteristics, as shown in Figure 1. […]
In recent years, the machining of mechanical parts is developing in the direction of intelligence and efficiency. With the increasing […]
The morphological characteristics of fracture reflect the quality of materials and play an important role in material quality inspection, fault […]
Under the influence of crack shape, the change of mode I stress intensity factor is studied. In the process of […]
The transmission system of shearer cutting part has the advantages of compact structure and high bearing capacity, and can realize […]
Under the action of cyclic load, cracks begin to appear and grow, and the remaining life of the sample is […]
Under the set parameters, the gear model is simulated. As shown in the figure, the trend distribution of stress intensity […]
By referring to the national standard GB / t6398-2000 test method for fatigue crack growth rate of metallic materials, the […]
The modeling module of ABAQUS software can effectively establish three-dimensional models, but most of them are suitable for three-dimensional model […]
(1) Present situation In the aspect of gear profile, because the involute gear has the advantages of convenient machining and […]
The fatigue crack evolution test and numerical simulation of transmission gears of heavy equipment are studied. The preparation of compact […]