Orthogonal experiment of spiral bevel gear
The test mainly investigates the influence of the grinding process parameters of spiral bevel gear (grinding depth, grinding speed and […]
The test mainly investigates the influence of the grinding process parameters of spiral bevel gear (grinding depth, grinding speed and […]
The spiral bevel gear of heavy vehicles generally adopts high-strength alloy steel such as 30CrMnTi. This kind of steel is […]
Surface roughness is not only the most important index to measure the surface morphology, but also an important standard to […]
The fixed grinding speed vs = 20.3 M / s and the spiral bevel gear speed VW = 1200 mm […]
The grinding test of spiral bevel gear on gleason-600g CNC gear grinding machine is designed. Firstly, the surface morphology of […]
The influence of different grinding parameters of gear steel materials on the surface residual stress has been discussed in detail. […]
(1) Experimental study on basic grinding of gear steel 30CrMnTi Referring to the actual processing conditions of spiral bevel gear, […]
After the spiral bevel gear is processed under given grinding conditions, the tooth surface has no obvious defects such as […]
Fixed spiral bevel gear speed VW = 1200 mm / min, grinding depth AP = 50 μ m. The test […]
The grinding parameters of spiral bevel gear arranged by single factor test are shown in the table. Parameters Value Grinding […]
Before grinding the spiral bevel gear used for the test, ensure the same machining process and its machining process as […]
Based on the accumulated Basic test data of surface grinding, the actual grinding test of spiral bevel gear on NC […]
The microhardness of workpiece grinding surface corresponding to different grinding speed and grinding depth of spiral bevel gear steel is […]
In the process of meshing transmission of spiral bevel gear, the surfaces of two teeth often need to contact and […]
The residual stress on the grinding surface plays a vital role in various properties of the workpiece. It has an […]
The variation law of grinding parameters on grinding force is studied, that is, the effects of grinding depth, grinding speed […]
Figure 1 shows the hardness change trend of the original sample without grinding of spiral bevel gear steel at different […]
Figure 1 shows the microstructure diagram of the section of the strengthening layer after grinding of 30crmnti. It can be […]
In order to observe the grinding strengthening layer of spiral bevel gear steel and the microstructure of the grinding surface, […]
For a long time, researchers at home and abroad hope to suppress and reduce the grinding heat generated in the […]
Referring to the actual processing conditions of spiral bevel gear, the basic test of surface grinding of gear steel material […]
The two-piece spiral bevel gear blank has been successfully formed by using the finite element numerical simulation method. In order […]
The research on the manufacturing technology of spiral bevel gear in China started relatively late. In 1971, Chinese researchers began […]
The precision forging die of spiral bevel gear is processed and assembled in Qingdao Sanxing precision forging gear factory, and […]
During grinding, grinding force will affect the formation of grinding heat and the performance of workpiece surface, and then have […]
In the 18th century, the French geometer T. Olivier first proposed the concept of spiral bevel gear, but due to […]
The spiral bevel gear blank formed by the two-piece ring rolling process, that is, the two spiral bevel gear blanks […]
The application of surface integrity index to comprehensively evaluate the surface machining quality of spiral bevel gear is of great […]
Heavy duty spiral bevel gear has many excellent characteristics, such as stable transmission performance, low noise, large transmission torque and […]
Friction between the metal die and the forging die is inevitable. Friction in metal plastic forming mainly has the following […]
Because the spiral bevel gear blank formed by the two-piece rolling process is a symmetrical figure, the 1/2 model is […]
As an important transmission part, the driven spiral bevel gear of automobile rear axle bears a large load, so the […]
Spiral bevel gear is widely used in automobile transmission system. Its transmission error is an important basis to evaluate the […]
Forming speed is also an important factor affecting the precision forging of spiral bevel gear. Because the process of plastic […]
To measure the standard of qualified spiral bevel gear blank, in addition to achieving the shape and dimensional accuracy, the […]
In order to investigate the influence of initial forging temperature on the precision forging of spiral bevel gear, the initial […]
The formed spiral bevel gear blank is formed by ring rolling based on the ring blank. Through numerical simulation of […]
Make full use of CAD two-dimensional software, CATIA three-dimensional software and DEFORM-3D finite element numerical simulation software to carry out […]
The ring rolling process of driven spiral bevel gear blank of automobile rear axle is analyzed. The forming of spiral […]
Before ring rolling, the formed spiral bevel gear blank has to go through four steps: pier roughening, pre punching, punching […]
Through a large number of numerical simulation experiments, on the basis of the theoretical calculation size of the ring blank, […]
As shown in the figure, the load stroke curve of precision forging of spiral bevel gear is shown. From the […]
The blank size of spiral bevel gear refers to the specific size of the material before the pier is rough, […]
The spiral bevel gear blank should be heated to 1150 ℃ for die forging, which belongs to hot die forging. […]
(1) Selection of diameter DP of spiral bevel gear blank Spiral bevel gear blank belongs to round cake forging, so […]
The forming temperature distribution of the bevel gear is reasonable, which has a great impact on the forming quality of […]
At present, the effective method to produce the driven spiral bevel gear blank of automobile rear axle at home and […]
Taking the automobile rear axle driven spiral bevel gear blank processed by ZHY gear as the research object, its original […]
Automobile rear axle is also called drive axle. It not only bears the load, but also acts as differential and […]
By comparing the advantages and disadvantages of various forming processes and combining the process methods of producing spiral bevel gear […]
Die forging refers to the method of using die processing to make the blank finally form the forging. This forging […]
Ring rolling process essentially belongs to plastic forming process. Through local deformation of spiral bevel gear blank, the overall forming […]
By analyzing the stress distribution in the forming process of spiral bevel gear forgings, we can fully understand the stress […]
As a transmission part, spiral bevel gear is widely used in automobile, machine tool, ship, aircraft and other related fields. […]
Strain is a physical quantity used to express the deformation size of the deformed body. Through the analysis of the […]
In 1674, Danish astronomer Romer used the enveloping cycloid as the gear tooth profile to obtain the gear with conjugate […]
Through the speed field of precision forging of spiral bevel gear, the flow of metal blank in the forming process […]
As shown in the table, the forging deformation force of open die forging and non flash die forging of spiral […]
Due to these irreplaceable advantages, spiral bevel gear has been widely used as an important part in the transmission system […]
(1) Mold and blank materials can be directly selected from the material library of DEFORM software. The mold material is […]