Obtaining spur gear parameters using machine vision
1.Obtaining Basic Gear Parameters There are many gear parameters and there are certain connections among them. The most important one […]
1.Obtaining Basic Gear Parameters There are many gear parameters and there are certain connections among them. The most important one […]
The hardness results of carburized layer of heat treated 2.3cr-0.9si-0.3mo steel were measured in the conversion gas reduction furnace and […]
Knowledge is the decisive factor of new product competitiveness. The product design based on knowledge engineering is to summarize and […]
The experimental results of ZHY gear only verify the correctness of the calculation method of tooth contact temperature under EHL […]
The abstract diagram of the cogwheel split torque drive is shown in Figure 1. The transmission direction shown in Figure […]
With the increasingly strict global regulations on carbon dioxide emissions and fuel consumption efficiency, automobile powertrain systems become more compact […]
The virtual design method of gearbox gear based on knowledge integrates knowledge engineering and parametric design technology, and develops the […]
According to the knock phenomenon of transmission gear, it is mainly divided into bench test and real vehicle test. In […]
With the all-round development of the mechanical industry, the requirements of the mechanical equipment for the transmission system are higher […]
The phenomenon of gear knocking in automobile transmission belongs to the NVH dynamics problem of transmission system. The research idea […]
Automobile transmission includes many pairs of helical gear pairs, multiple bearings and synchronizer assemblies, etc. when considering the spatial meshing […]
With the rapid development of the automobile industry, automobile users have higher and higher requirements for the comfort of automobile […]
The figure shows the gear drive with the number of teeth (Z1=31, Z2=32), modulus (m=6), pressure angle (a=20 degrees), crest […]
The diagram shows the variation trend of gear crest height coefficient when the number of teeth (Z1=31, Z2=32), modulus (m=6), […]
Figure 1 shows the change trend of the sliding rate with the number of teeth (transmission ratio) of the gear […]
Theoretically, when k is engaged at N2, η 2 = ∞, η 1 = – 1; when k is engaged […]
The ratio of the relative tangential speed of the gear pair between the tooth surfaces at the meshing point and […]
Gear, as a widely used mechanical component in mechanical transmission, has the characteristics of accurate transmission ratio, high bearing capacity […]
Laser cutting equipment mainly uses heat energy generated by laser beam emitted by laser to cut pipes with motion mechanical […]
As an additive manufacturing technology, 3D printing is a new technology that subverts the traditional manufacturing, and has become the […]
In order to reflect the influence rule of parameters on the maximum circumferential stress, dimensionless radius of chamfered root of […]
Because the former three machining methods are based on the simulation of meshing between the small wheel (or the profile […]
1. Maximum circumferential stress of ring gear in design specification Considering the influence of tooth parameters, load distortion of flexible […]
Dr. Stadtfeld of Greenson first outlined the idea of using disc wheel to machine face gear. It has the advantages […]
In view of the distortion caused by various factors, such as the release of processing stress, the different time and […]
1. Basic profile parameters and definitions Taking the involute profile as an example, Figure shows an illustration of the involute […]
1. Gear Fracture and Analysis According to user feedback, the gear breaks under heavy load and the fracture occurs in […]
A gear tooth with fracture failure was randomly selected for fracture analysis. The fracture was cut off by wire cutting […]
Generally, the heat treatment distortion of the controlled workpiece is focused on “quenching distortion”. The reason is that the quenching […]
According to the analysis of the cutting process of spiral bevel gear tooth surface, based on the generation principle of […]
The meshing frequency and its double frequency of each pair of wheels constitute the main vibration excitation components of the […]
Based on the analysis of the cutting principle of the tooth surface of the spherical involute involute involute spiral bevel […]
The dynamic load of the system is calculated when the speed is 500r / min and the load is 500N […]
This paper takes the concave tooth surface of right-hand spiral bevel gear as an example to analyze and study the […]
Planetary gear drive is widely used in various industrial fields due to its large power weight ratio, high load-carrying capacity […]
In order to intuitively analyze the generation principle of right spiral bevel gear convex tooth surface, the method of establishing […]
There are two main machining methods of spiral bevel gears, forming method and generating method. Forming method The profile of […]
The total empty return of the gear transmission chain caused by the factors such as the increase of the gear […]
Traditional spiral bevel gear machining is based on the principle of “imaginary flat top gear”. At present, the basic idea […]
Gear is the core and basic component of mechanical transmission equipment. Under the dynamic excitation, it will produce dynamic response […]
Spiral bevel gear is widely used in various mechanical products such as aircraft, ship and national defense equipment, machine tools, […]
Gear transmission is one of the most important mechanical transmission. More than 300 BC, Aristotle, the ancient Greek philosopher, expounded […]
In addition to the lubrication of gears and bearings, ATF is also used for the lubrication and cooling of hydraulic […]
An important research direction of gear geometry is noncircular gear transmission. Its complex tooth surface geometry and special transmission performance […]
The thermal behavior of the high-speed and heavy-duty gear system has a great influence on its bearing capacity. In the […]
1. Spraying technology of superfine composite materials In recent years, Chinese and Japanese companies have studied and applied the spraying […]
The machining method of the eccentric modification gear generated by the modification method is the same as that of the […]
Gear transmission system is the core mechanism of mechanical equipment, which determines the performance of the whole machine. But for […]
Molybdenum disulfide (MoS2), as a high quality solid lubricating material, has good antifriction, antiwear and bearing capacity. Molybdenum disulfide (MoS2) […]
The transmission between the eccentric gears will produce the change of backlash. Therefore, when calculating the coefficient of deflection of […]
The application of manganese phosphate conversion coating technology in improving the surface strength of transmission parts first appeared in improving […]
According to the statistical analysis of the faults, it is found that the gears and bearings on the second shaft […]
As one of the main equipment of the coal mining face, the shearer is required to have high reliability in […]
The strengthening technology of gear heat treatment should pay attention to the control of surface integrity, that is, to control […]
The automobile gear is in the state of continuous load operation. There are rolling and sliding between the meshing surfaces […]
Gear is an important part to transmit power in mechanical devices. The Japanese mechanical society has carried out systematic investigation […]
According to the above analysis, in order to thoroughly solve the undercut fracture accident of thin-walled gear and ensure the […]
According to the failure mechanism analysis of thin-walled gear, the gear material is 40Mn2. In the process of gear meshing, […]
As the key part to change the driving direction and keep the vehicle running in a stable straight line, the […]
It is found that the broken tooth thin-walled gear is a 2 ″ straight cylindrical gear with 12 teeth, which […]